Which steel is easiest to machine? This machinability ranking lists 34 carbon and low alloy steels in the annealed condition by machining speed, plus 21 grades that are only available in other conditions and the precipitation hardening stainless steels on our site. Machining speed, hardness and tensile strength are taken from our material data sheets; each grade links to its data sheet.
Machining speed in these data sheets is a reference cutting speed in metres per minute: a higher value means the material can be cut faster. Hardness and condition matter as much as the grade, so the tables show both.
Steel Machinability Ranking: Annealed Condition
| Rank | Grade | Type | Machining speed (m/min) | Hardness (HV) | Tensile strength (MPa) |
|---|---|---|---|---|---|
| 1 | AISI 1010 | Low Carbon Steel | 45.7 | 88–128 | 310–430 |
| 1 | AISI 1015 | Low Carbon Steel | 45.7 | 108–128 | 345–430 |
| 1 | AISI 1020 | Low Carbon Steel | 45.7 | 110–130 | 355–435 |
| 1 | AISI 1117 | Resulfurized Low Carbon Steel | 45.7 | 118–140 | 385–475 |
| 1 | AISI 1118 | Resulfurized Low Carbon Steel | 45.7 | 128–150 | 405–495 |
| 1 | AISI 1144 | Resulfurized Medium Carbon Steel | 45.7 | 155–190 | 525–645 |
| 7 | AISI 1022 | Low Carbon Steel | 39.6 | 130–160 | 380–475 |
| 7 | AISI 1030 | Medium Carbon Steel | 39.6 | 120–145 | 410–515 |
| 9 | AISI 1137 | Resulfurized Medium Carbon Steel | 36.6 | 160–200 | 520–645 |
| 9 | AISI 1141 | Resulfurized Medium Carbon Steel | 36.6 | 150–190 | 540–660 |
| 11 | AISI 1040 | Medium Carbon Steel | 33.5 | 143–173 | 475–575 |
| 11 | AISI 8620 | Low Alloy Steel | 33.5 | 140–170 | 480–595 |
| 13 | AISI 4620 | Low Alloy Steel | 30.5 | 140–170 | 460–560 |
| 13 | AISI 8630 | Low Alloy Steel | 30.5 | 145–180 | 500–625 |
| 15 | AISI 4130 | Low Alloy Steel | 29.9 | 145–185 | 500–620 |
| 15 | AISI 5140 | Low Alloy Steel | 29.9 | 155–190 | 510–635 |
| 17 | AISI 4320 | Low Alloy Steel | 28.3 | 150–190 | 520–640 |
| 18 | AISI 1080 | High Carbon Steel | 27.7 | 160–200 | 550–680 |
| 19 | AISI 1060 | Medium Carbon Steel | 27.4 | 165–205 | 550–700 |
| 20 | AISI 1050 | Medium Carbon Steel | 26.8 | 173–213 | 570–705 |
| 21 | AISI 5150 | Low Alloy Steel | 25.9 | 160–230 | 605–750 |
| 22 | AISI 1340 | Medium Carbon Manganese Steel | 25.6 | 190–235 | 630–775 |
| 23 | AISI 4140 | Low Alloy Steel | 25 | 183–223 | 595–720 |
| 23 | AISI 6150 | Low Alloy Steel | 25 | 183–225 | 595–740 |
| 25 | AISI 3140 | Low Alloy Steel | 24.4 | 185–225 | 620–760 |
| 26 | AISI 1095 | High Carbon Steel | 24.1 | 180–220 | 590–720 |
| 26 | AISI 5160 | Low Alloy Steel | 24.1 | 183–225 | 645–800 |
| 28 | AISI 4150 | Low Alloy Steel | 23.8 | 183–223 | 660–800 |
| 28 | AISI 8740 | Low Alloy Steel | 23.8 | 185–230 | 625–765 |
| 30 | AISI 4820 | Low Alloy Steel | 22.9 | 183–223 | 610–750 |
| 31 | AISI 8650 | Low Alloy Steel | 22.6 | 193–243 | 640–790 |
| 32 | AISI 4340 | Low Alloy Steel | 21.3 | 200–245 | 670–820 |
| 32 | AISI 9255 | Low Alloy Steel | 21.3 | 210–260 | 695–855 |
| 34 | AISI 9310 | Low Alloy Steel | 18.6 | 220–270 | 735–905 |
■ carbon steels ■ low alloy steels
Machinability of Grades Without Annealed Data
These grades have no annealed data sheet on our site, so the table shows the condition with the highest machining speed among their available data sheets. Compare them with the annealed ranking with the condition in mind.
Machinability of Precipitation Hardening Stainless Steels
For the precipitation hardening stainless steels on our site, the table shows the fastest and slowest machining speed among the available conditions of each grade.
| Grade | Fastest condition (m/min) | Slowest condition (m/min) |
|---|---|---|
| 15-5PH | H1150M (14.9) | H900 (12.2) |
| 17-4PH | H1150M (14.9) | H900 (12.2) |
| Custom 450 | ST (14.9) | H900 (10.4) |
| FV520 | primary and secondary hardened at 540°C (BS S143) (12.8) | hardened at 450°C (BS S145) (9.45) |
| AM-350 | SCT 850 (11.3) | SCT 850 (11.3) |
| AM-355 | SCT 1000 (11.3) | SCT 850 (10.7) |
| 17-7PH | TH1050 (10.4) | TH1050 (10.4) |
| PH15-7Mo | TH1050 (9.75) | TH1050 (9.75) |
| PH 13-8Mo | H1150 (9.14) | H950 (7.62) |
| Custom 455 | H1000 (8.84) | H950 (7.92) |
| Custom 465 | H1000 (7.01) | H950 (6.71) |
How Heat Treatment Changes Machining Speed
| Grade | Annealed | Normalized | Oil Q&T 650°C | Oil Q&T 205°C |
|---|---|---|---|---|
| AISI 1040 | 33.5 | 29.3 | 26.2 | 20.1 |
| AISI 4140 | 25 | 15.8 | 21.3 | 8.84 |
| AISI 4340 | 21.3 | 12.2 | 16.2 | 8.23 |
In the annealed condition the highest machining speed in our data, 45.7 m/min, is shared by AISI 1010, AISI 1015, AISI 1020, AISI 1117, AISI 1118 and AISI 1144; the lowest is AISI 9310 (18.6 m/min). Within one grade, machining speed falls as hardness rises: in the table above, the oil quenched and tempered at 205°C condition cuts at 35–60% of the annealed speed.
Steel Machinability FAQ
In the annealed condition the highest machining speed in our data sheets is 45.7 m/min, shared by AISI 1010, AISI 1015, AISI 1020, AISI 1117, AISI 1118 and AISI 1144.
Among the annealed low alloy steels in our data, AISI 8620 has the highest machining speed (33.5 m/min) and AISI 9310 the lowest (18.6 m/min).
Annealed AISI 4140 has a machining speed of 25 m/min in our data sheet. Quenched and tempered, it falls to 8.84 m/min at 205°C and 21.3 m/min at 650°C.
Yes. Within one grade, machining speed falls as hardness rises. In our data, oil quenched and tempered at 205°C material cuts at roughly 35–60% of the annealed speed for AISI 1040, 4140 and 4340.
In our data sheets the highest machining speed among the PH stainless steels is 14.9 m/min, reached by 15-5PH H1150M, 17-4PH H1150M and Custom 450 ST.
Related: resulfurized free-machining steels compared | steel tempering chart | low carbon steel grades | low alloy steel grades
Need machined steel parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined carbon steel, low alloy steel and stainless steel parts in-house and inspects them before shipment.