| Mechanical properties | Values |
|---|---|
| Young’s modulus | 193 – 201 GPa |
| Specific stiffness | 24.7 – 25.9 MN.m/kg |
| Yield strength (elastic limit) | 275 – 350 MPa |
| Tensile strength | 655 – 950 MPa |
| Specific strength | 35.2 – 44.9 kN.m/kg |
| Elongation | 40 – 45 % strain |
| Compressive strength | * 275 – 515 MPa |
| Flexural modulus | * 193 – 201 GPa |
| Flexural strength (modulus of rupture) | 275 – 515 MPa |
| Shear modulus | 75 – 80 GPa |
| Poisson’s ratio | 0.265 – 0.275 |
| Shape factor | 59 |
| Hardness – Vickers | * 180 – 208 HV |
| Hardness – Rockwell B | 85 – 95 HRB |
| Hardness – Rockwell C | * 4 – 15 HRC |
| Hardness – Brinell | 217 – 245 HB |
| Elastic stored energy (springs) | 1.45e3 – 2.16e3 kJ/m^3 |
| Fatigue strength at 10^7 cycles | * 268 – 386 MPa |
| Fatigue strength model (stress range) | * 221 – 468 MPa |
| *Values indicated with asterisks (*) are approximate. No guarantee is provided for the precision of this information. |