AISI 1020 Low Carbon Steel

AISI 1020 Low Carbon Steel

AISI 1020 Steel Overview

AISI 1020 steel (UNS G10200) is a low carbon steel. This page lists the AISI 1020 material data sheets for 3 conditions: annealed, as rolled, normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 1020 Steel

Forgings, machined parts, shafts, car wheel hubs, general haulage gear

AISI 1020 Steel Chemical Composition

C (carbon)0.17 – 0.23 %
Fe (iron)99.1 – 99.5 %
Mn (manganese)0.3 – 0.6 %
P (phosphorus)0 – 0.04 %
S (sulfur)0 – 0.05 %

AISI 1020 Steel Material Data Sheets

AISI 1020 Annealed Material Data Sheet

AISI 1020 As Rolled Material Data Sheet

AISI 1020 Normalized Material Data Sheet

AISI 1020 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 1020 Annealed vs As Rolled vs Normalized: Yield, Tensile & Hardness Compared.

AISI 1020 Steel Parts from Turkey

Looking for AISI 1020 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1020 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low carbon steel grades.