We are a supplier and service company specializing in the assembly of parts using adhesives. At Modulus Metal, we offer a wide range of adhesives to meet the specific needs of our customers.
FLEXIBLE adhesives are ideal for bonding materials that may experience movement or vibration.
Some examples of flexible adhesives that we offer include:
- Neoprene: a synthetic rubber adhesive that is resistant to oil, weather, and ageing
- Nitrile: an adhesive made from a copolymer of acrylonitrile and butadiene, known for its high resistance to oil and fuels
- Polyurethane: a strong and flexible adhesive that is resistant to abrasion and impact
- Silicones: a family of adhesives known for their high-temperature resistance and flexibility
RIGID adhesives are best suited for bonding materials that will not experience movement or vibration.
Some examples of rigid adhesives that we offer include:
- Acrylic: a strong and durable adhesive that is resistant to water and UV light
- Anaerobic: an adhesive that cures in the absence of oxygen, ideal for bonding metal parts
- Cyanoacrylates: a fast-setting adhesive that is resistant to water and chemicals
- Epoxy: a strong and durable adhesive that is resistant to heat and chemicals
- Inorganic: an adhesive made from inorganic materials, such as ceramics or glass
- Phenolic: an adhesive made from phenol and formaldehyde, known for its high heat resistance
- Polyester: a strong and durable adhesive that is resistant to UV light and water
- Polysulfide: an adhesive that is resistant to water, fuels, and oils
SOLVENT BONDING is a method of bonding materials by using a solvent to soften and dissolve the surfaces to be joined. This method is often used when bonding materials that are not compatible with other adhesives.
At Modulus Metal, we have the expertise and equipment necessary to assemble parts using the appropriate adhesive for your specific needs. Whether you are in need of a small batch of parts or a large volume, we have the capability to meet your needs.
Thank you for considering Modulus Metal for your adhesive assembly needs. If you have any questions or would like to discuss your project in more detail, please don’t hesitate to contact us.

USEFUL INFO
List of EN Standards for Adhesives:
| Standard No | Standard |
|---|---|
| EN 204:2016 | Classification of thermoplastic wood adhesives for non-structural applications |
| EN 205:2016 | Adhesives – Wood adhesives for non-structural applications – Determination of tensile shear strength of lap joints |
| EN 301:2013 | Adhesives, phenolic and aminoplastic, for load-bearing timber structures – Classification and performance requirements |
| EN 302-1:2013 | Adhesives for load-bearing timber structures – Test methods – Part 1: Determination of longitudinal tensile shear strength |
| EN 302-2:2017 | Adhesives for load-bearing timber structures – Test methods – Part 2: Determination of resistance to delamination |
| EN 302-3:2017 | Adhesives for load-bearing timber structures – Test methods – Part 3: Determination of the effect of acid damage to wood fibres by temperature and humidity cycling on the transverse tensile strength |
| EN 302-4:2017 | Adhesives for load-bearing timber structures – Test methods – Part 4: Determination of the effects of wood shrinkage on the shear strength |
| EN 302-5:2013 | Adhesives for load-bearing timber structures – Test methods – Part 5: Determination of maximum assembly time under referenced conditions |
| EN 302-6:2013 | Adhesives for load-bearing timber structures – Test methods – Part 6: Determination of the minimum pressing time under referenced conditions |
| EN 302-7:2013 | Adhesives for load-bearing timber structures – Test methods – Part 7: Determination of the working life under referenced conditions |
| EN 302-8:2017 | Adhesives for load-bearing timber structures – Test methods – Part 8: Static load test of multiple bond line specimens in compression shea |
| EN 542:2003 | Adhesives – Determination of density |
| EN 543:2003 | Adhesives – Determination of apparent density of powder and granule adhesives |
| EN 827:2005 | Adhesives – Determination of conventional solids content and constant mass solids content |
| EN 828:2013 | Adhesives – Wettability – Determination by measurement of contact angle and surface free energy of solid surface |
| EN 923:2015 | Adhesives – Terms and definitions |
| EN 924:2003 | Adhesives – Solvent-borne and solvent-free adhesives – Determination of flashpoint |
| EN 1067:2005 | Adhesives – Examination and preparation of samples for testing |
| EN 1238:2011 | Adhesives – Determination of the softening point of thermoplastic adhesives (ring and ball) |
| EN 1239:2011 | Adhesives – Freeze-thaw stability |
| EN 1240:2011 | Adhesives – Determination of hydroxyl value and/or hydroxyl content |
| EN 1241:1998 | Adhesives – Determination of acid value |
| EN 1242:2013 | Adhesives – Determination of isocyanate content |
| EN 1243:2011 | Adhesives – Determination of free formaldehyde in amino and amidoformaldehyde condensates |
| EN 1244:1998 | Adhesives – Determination of the colour and/or colour changes of adhesive coats under the influence of light |
| EN 1245:2011 | Adhesives – Determination of pH |
| EN 1246:1998 | Adhesives – Determination of ash and sulphated ash |
| EN 1372:2015 | Adhesives – Test method for adhesives for floor and wall coverings – Peel test |
| EN 1373:2015 | Adhesives – Test method for adhesives for floor and wall coverings – Shear test |
| EN 1392:2006 | Adhesives for leather and footwear materials-Solvent-based and dispersion adhesives-Testing of bond strength under specified conditions |
| EN 1464:2010 | Adhesives – Determination of peel resistance of adhesive bonds – Floating roller method |
| EN 1465:2009 | Adhesives – Determination of tensile lap-shear strength of bonded assemblies |
| EN 1719:1998 | Adhesives for paper and board, packaging and disposable sanitary products – Tack measurement for pressure sensitive adhesives – Determination of loop tack |
| EN 1720:1998 | Adhesives for paper and board, packaging and disposable sanitary products – Determination of dispersability |
| EN 1721:1998 | Adhesives for paper and board, packaging and disposable sanitary products – Track measurement for pressure sensitive adhesives – Determination of rolling ball track |
| EN 1841:1998 | Adhesives – Test methods for adhesives for floor coverings and wall coverings – Determination of dimensional changes of a linoleum floor covering in contact with an adhesive |
| EN 1895:2001 | Adhesives for paper and board, packaging and disposable sanitary products – 180° – “T” peel test for a flexible-to-flexible assembly |
| EN 1895:2001/AC:2007 | Adhesives for paper and board, packaging and disposable sanitary products – 180°-“T” peel test for a flexible-to-flexible assembly |
| EN 1896:2001 | Adhesives for paper and board, packaging and disposable sanitary products – Determination of tensile strength and elongation |
| EN 1902:2015 | Adhesives – Test method for adhesives for floor and wall coverings – Shear creep test |
| EN 1903:2015 | Adhesives – Test method for adhesives for plastic or rubber floor coverings or wall coverings – Determination of dimensional changes after accelerated ageing |
| EN 1937:1999 | Test method for hydraulic setting floor smoothing and/or levelling compounds – Standard mixing procedures |
| EN 1939:2003 | Self adhesive tapes – Determination of peel adhesion properties |
| EN 1942:2008 | Self adhesive tapes – Measurement of Thickness |
| EN 1943:2002 | Self adhesive tapes – Measurement of static shear adhesion |
| EN 1944:1996 | Self-adhesive tapes – Measurement of unwind adhesion at low speed |
| EN 1945:1996 | Self-adhesive tapes – Measurement of quick stick |
| EN 1965-1:2011 | Structural adhesives – Corrosion – Part 1: Determination and classification of corrosion to a copper substrate |
| EN 1965-2:2011 | Structural adhesives – Corrosion – Part 2: Determination and classification of corrosion to a brass substrate |
| EN 1966:2009 | Structural adhesives – Characterization of a surface by measuring adhesion by means of the three point bending method |
| EN ISO 8510-2:2010 | Adhesives – Peel test for a flexible-bonded-to-rigid test specimen assembly – Part 2: 180 degree peel (ISO 8510-2:2006) |
| EN ISO 9142:2003 | Adhesives – Guide to the selection of standard laboratory ageing conditions for testing bonded joints (ISO 9142:2003) |
| EN ISO 9311-1:2005 | Adhesives for thermoplastic piping systems – Part 1: Determination of film properties (ISO 9311-1:2005) |
| EN ISO 9311-2:2011 | Adhesives for thermoplastic piping systems – Part 2: Determination of shear strength (ISO 9311-2:2011) |
| EN ISO 9311-3:2005 | Adhesives for thermoplastic piping systems – Part 3: Test method for the determination of resistance to internal pressure (ISO 9311-3:2005) |
| EN ISO 9653:2000 | Adhesives – Test method for shear impact strength of adhesive bonds (ISO 9653:1998) |
| EN ISO 9664:1995 | Adhesives – Test methods for fatigue properties of structural adhesives in tensile shear (ISO 9664:1993) |
| EN ISO 9665:2000 | Adhesives – Animal glues – Methods of sampling and testing (ISO 9665:1998) |
| EN ISO 10363:1995 | Hot-melt adhesives – Determination of thermal stability (ISO 10363:1992) |
| EN ISO 10365:1995 | Adhesives – Designation of main failure patterns (ISO 10365:1992) |
| EN ISO 11339:2010 | Adhesives – T-peel test for flexible-to-flexible bonded assemblies (ISO 11339:2010) |
| EN ISO 11343:2005 | Adhesives – Determination of dynamic resistance to cleavage of high-strength adhesive bonds under impact conditions – Wedge impact method (ISO 11343:2003) |
| EN 12023:1996 | Self-adhesive tapes – Measurement of water transmission in a warm humid atmosphere |
| EN 12024:1996 | Self-adhesive tapes – Measurement of resistance to elevated temperature and humidity |
| EN 12025:1996 | Self-adhesive tapes – Measurement of tear resistance by the pendulum |
| EN 12026:1996 | Self-adhesive tapes – Measurement of the unwinding force at high speed |
| EN 12027:1996 | Self-adhesive tapes – Measurement of flame resistance |
| EN 12028:1996 | Self-adhesive tapes – Measurement of elongation under static load |
| EN 12029:1996 | Self-adhesive tapes – Determination of the water-soluble corrosive ions |
| EN 12030:1996 | Self-adhesive tapes – Measurement of impact resistance |
| EN 12031:1996 | Self-adhesive tapes – Measurement of bursting strength |
| EN 12032:1996 | Self-adhesive tapes – Measurement of bonding of thermosetting adhesive tapes during curing |
| EN 12033:1996 | Self-adhesive tapes – Measurement of bonding of thermosetting adhesive tapes after curing |
| EN 12034:1996 | Self-adhesive tapes – Measurement of the length of a roll of adhesive tape |
| EN 12035:1996 | Self-adhesive tapes – Flagging of adhesive tape |
| EN 12036:1996 | Self-adhesive tapes – Solvent penetration into adhesive masking tapes |
| EN 12092:2001 | Adhesives – Determination of viscosity |
| EN 12436:2001 | Adhesives for load-bearing timber structures – Casein adhesives – Classification and performance requirements |
| EN 12481:2000 | Self adhesive tapes – Terminology |
| EN 12701:2001 | Structural adhesives – Storage – Determination of words and phrases relating to the product life of structural adhesives and related materials |
| EN 12702:2000 | Adhesives for paper and board, packaging and disposable sanitary products – Determination of blocking behaviour of potentially adhesive layers |
| EN 12703:2016 | Adhesives for paper and board, packaging and disposable sanitary products – Determination of low temperature flexibility or cold crack temperature |
| EN 12704:2016 | Adhesives for paper and board, packaging and disposable sanitary products – Determination of foam formation for aqueous adhesives |
| EN 12705:2011 | Adhesives for leather and footwear materials – Determination of colour change of white or bright coloured leather surfaces by migration |
| EN 12706:1999 | Adhesives – Test methods for hydraulic setting floor smoothing and/or levelling compounds – Determination of flow characteristics |
| EN 12765:2016 | Classification of thermosetting wood adhesives for non-structural applications |
| EN 12960:2001 | Adhesives for paper and board, packaging and disposable sanitary products – Determination of shear resistance |
| EN 12960:2001/AC:2007 | Adhesives for paper and board, packaging and disposable sanitary products – Determination of shear resistance |
| EN 12961:2001 | Adhesives for leather and footwear materials – Determination of optimum activation temperatures and maximum activation life of solvent-based and dispersion adhesives |
| EN 12961:2001/A1:2005 | Adhesives for leather and footwear materials – Determination of optimum activation temperatures and maximum activation life or solvent-based and dispersion adhesives |
| EN 12962:2011 | Adhesives – Determination of elastic behaviour of liquid adhesives (elasticity index) |
| EN 12963:2001 | Adhesives – Determination of free monomer content in adhesives based on synthetic polymers |
| EN 12964:2001 | Adhesives for leather and footwear materials – Lasting adhesives – Testing heat resistance of bonds at increasing temperature |
| EN 13408:2002 | Methods of test for hydraulic setting floor smoothing and/or levelling compounds – Determination of bond strength |
| EN 13409:2002 | Methods of test for hydraulic setting floor smoothing and/or levelling compounds – Determination of setting time |
| EN 13415:2010 | Test of adhesives for floor covering – Determination of the electrical resistance of adhesive films and composites |
| EN ISO 13445:2006 | Adhesives – Determination of shear strength of adhesive bonds between rigid substrates by the block-shear method (ISO 13445:2003) |
| EN 13872:2004 | Methods of test for hydraulic setting floor smoothing and/or levelling compounds – Determination of dimensional change |
| EN 13887:2003 | Structural Adhesives – Guidelines for surface preparation of metals and plastics prior to adhesive bonding |
| EN 13999-1:2013 | Adhesives – Short term method for measuring the emission properties of low-solvent or solvent-free adhesives after application – Part 1: General procedure |
| EN 13999-2:2013 | Adhesives – Short term method for measuring the emission properties of low-solvent or solvent-free adhesives after application – Part 2: Determination of volatile organic compounds |
| EN 13999-3:2007+A1:2009 | Adhesives – Short term method for measuring the emission properties of low-solvent or solvent-free adhesives after application – Part 3: Determination of volatile aldehydes |
| EN 13999-4:2007+A1:2009 | Adhesives – Short term method for measuring the emission properties of low-solvent or solvent-free adhesives after application – Part 4: Determination of volatile diisocyanates |
| EN 14022:2010 | Structural Adhesives – Determination of the pot life (working life) of multi-component adhesives |
| EN 14256:2007 | Adhesives for non-structural wood applications – Test method and requirements for resistance to static load |
| EN 14257:2006 | Adhesives – Wood adhesives – Determination of tensile strength of lap joints at elevated temperature (WATT ’91) |
| EN 14258:2004 | Structural adhesives – Mechanical behaviour of bonded joints subjected to short and long terms exposure at specified conditions of temperature |
| EN 14259:2003 | Adhesives for floor coverings – Requirements for mechanical and electrical performance |
| EN 14292:2005 | Adhesives – Wood adhesives – Determination of static load resistance with increasing temperature |
| EN 14293:2006 | Adhesives – Adhesives for bonding parquet to subfloor – Test methods and minimum requirements |
| EN 14294:2010 | Adhesives for leather and footwear materials – Preparation of bonded test pieces by moulding-on processes |
| CR 14376:2002 | Adhesives – Adhesives for paper and board, packaging and disposable sanitary products – Description and assessment of the setting process |
| EN 14410:2003 | Self adhesive tapes – Measurement of breaking strength and elongation at break |
| EN 14444:2005 | Structural adhesives – Qualitative assessment of durability of bonded assemblies – Wedge rupture test (ISO 10354:1992 modified) |
| EN 14444:2005/AC:2008 | Structural adhesives – Qualitative assessment of durability of bonded assemblies – Wedge rupture test (ISO 10354:1992 modified) |
| EN 14510:2005 | Adhesives for leather and footwear materials – Solvent-based and dispersion adhesives – Determination of sole positioning tack (spotting tack) |
| EN ISO 14678:2005 | Adhesives – Determination of resistance to flow (sagging) (ISO 14678:2005) |
| EN 14680:2015 | Adhesives for non-pressure thermoplastics piping systems – Specifications |
| EN 14713:2016 | Adhesives for paper and board, packaging and disposable sanitary products – Determination of friction properties of films potentially suitable for bonding |
| EN 14814:2016 | Adhesives for thermoplastic piping systems for fluids under pressure – Specifications |
| EN 14869-1:2011 | Structural adhesives – Determination of shear behaviour of structural bonds – Part 1: Torsion test method using butt-bonded hollow cylinders (ISO 11003-1:2001, modified) |
| EN 14869-2:2011 | Structural adhesives – Determination of shear behaviour of structural bonds – Part 2: Thick adherends shear test (ISO 11003-2:2001, modified) |
| CEN/TS 14999:2013 | Adhesives for thermoplastic piping systems – Accelerated ageing test in storage container |
| EN 15062:2006 | Adhesives for leather and footwear materials – Solvent-based and dispersion adhesives – Testing ageing of bonds under specified conditions |
| EN 15190:2007 | Structural adhesives – Test methods for assessing long term durability of bonded metallic structures |
| EN 15274:2015 | General purpose adhesives for structural assembly – Requirements and test methods |
| EN 15275:2015 | Structural adhesives – Characterisation of anaerobic adhesives for co-axial metallic assembly in building and civil engineering structures |
| EN 15307:2014 | Adhesives for leather and footwear materials – Sole-upper bonds – Minimum strength requirements |
| EN 15336:2007 | Adhesives – Determination of the time to rupture of bonded joints under static load ( ISO 15109:1998 modified) |
| EN 15337:2007 | Adhesives – Determination of shear strength of anaerobic adhesives using pin-and-collar specimens (ISO 10123:1990 modified) |
| EN 15416-1:2017 | Adhesives for load bearing timber structures other than phenolic and aminoplastic – Test methods – Part 1: Long-term tension load test perpendicular to the bond line at varying climate conditions with specimens perpendicular to the glue line (Glass house |
| EN 15416-2:2007 | Adhesives for load bearing timber structures other than phenolic and aminoplastic – Test methods – Part 2: Static load test of multiple bondline specimens in compression shear |
| EN 15416-3:2017 | Adhesives for load bearing timber structures other than phenolic and aminoplastic – Test methods – Part 3: Creep deformation test at cyclic climate conditions with specimens loaded in bending shear |
| EN 15416-4:2017 | Adhesives for load bearing timber structures other than phenolic and aminoplastic – Test methods – Part 4: Determination of open assembly time for one component polyurethane adhesives |
| EN 15416-5:2017 | Adhesives for load bearing timber structures other than phenolic and aminoplastic – Test methods – Part 5: Determination of conventional pressing time |
| EN 15425:2017 | Adhesives – One component polyurethane for load bearing timber structures – Classification and performance requirements |
| EN ISO 15605:2004 | Adhesives – Sampling (ISO 15605:2000) |
| EN 15865:2009 | Adhesives – Determination of torque strength of anaerobic adhesives on threaded fasteners (ISO 10964:1993 modified) |
| EN 15870:2009 | Adhesives – Determination of tensile strength of butt joints (ISO 6922:1987 modified) |
| EN ISO 15908:2002 | Adhesives for thermoplastic piping systems – Test method for the determination of thermal stability of adhesives (ISO 15908:2002) |
| CEN/TR 15990:2010 | Data Sheets – Footwear Tests Materials and Test Adhesives |
| CEN/TR 15990:2010/AC:2010 | Data Sheets – Footwear Tests Materials and Test Adhesives |
| EN 16254:2013+A1:2016 | Adhesives – Emulsion polymerized isocyanate (EPI) for load-bearing timber structures – Classification and performance requirements |
| EN 16556:2014 | Determination of the maximum open time for thermoplastic wood adhesives for non-structural applications |
| EN 28510-1:2014 | Adhesives – Peel test for a flexible-bonded-to-rigid test specimen assembly – Part 1: 90º peel |