ISO 9013 Thermal Cutting Dimensional Tolerances

Typically achievable limit deviation classes for cutting processes

ProcessClass
Laser cutting (up to 32 mm)1
oxyfuel flame cutting2
Plasma cutting2

Limit deviations for nominal dimensions tolerance class 1 (Dimensions in millimetres)

Work piece thickness
a
Nominal dimensions
>0 to <3≥3 to <10≥10 to <35≥35
to <125
≥125
to <315
≥315
to <1 000
≥1000
to <2 000
≥2 000
to <4 000
≥4 000
to <6 000
≥6 000
to <8 000
Limit deviations
>0to ≤1±0.075±0.10±0.10±0.20±0.20±0.30±0.40±0.65±0.90±1.60
>1to ≤3.15±0.10±0.15±0.20±0.25±0.25±0.35±0.40±0.65±1.00±1.75
>3.15to ≤6.3±0.20±0.20±0.25±0.25±0.30±0.40±0.45±0.70±1.10±1.90
>6.3to ≤10–±0.25±0.30±0.30±0.35±0.45±0.55±0.75±1.25±2.20
>10to ≤15–±0.30±0.35±0.40±0.45±0.55±0.65±0.85±1.50±2.50
>15to ≤20–±0.40±0.40±0.45±0.55±0.75±0.85±1.2±1.90±2.80
>20to ≤25–±0.45±0.50±0.60±0.70±0.90±1.10±1.60±2.40±3.25
>25to ≤32––±0.70±0.70±0.80±1.0±1.6±2.25±3.00±4.00
>32to ≤50––±0.7±0.70±0.8±1.0±1.6±2.5±3.8±5.0
>50to ≤100––±1.3±1.3±1.4±1.7±2.2±3.1±4.4±5.6
>100to ≤150––±1.9±2.0±2.1±2.3±2.9±3.8±5.1±6.3
>150to ≤200––±2.6±2.7±2.7±3.0±3.6±4.5±5.7±7.0
>200to ≤250–––––±3.7±4.2±5.2±6.4±7.7
>250to ≤300–––––±4.4±4.9±5.9±7.1±8.4

Limit deviations for nominal dimensions tolerance class 2 (Dimensions in millimetres)

Work piece thickness
a
Nominal dimensions
>0 to <3≥3 to <10≥10 to <35≥35
to <125
≥125
to <315
≥315
to <1 000
≥1000
to <2 000
≥2 000
to <4 000
≥4 000
to <6 000
≥6 000
to <8 000
Limit deviations
>0to ≤1±0.5±0.6±0.6±0.7±0.7±0.8±0.9±0.9––
>1to ≤3,15±0.6±0.6±0.7±0.7±0.8±0.9±1±1.1±1.4±1.4
>3,15to ≤6,3±0.7±0.8±0.9±0.9±1.1±1.2±1.3±1.3±1.6±1.6
>6,3to ≤10–±1±1.1±1.3±1.4±1.5±1.6±1.7±1.9±2
>10to ≤15–±1.8±1.8±1.8±1.9±2.3±3±4.2±4.3±4.5
>15to ≤20–±1.8±1.8±1.8±1.9±2.3±3±4.2±4.3±4.5
>20to ≤25–±1.8±1.8±1.8±1.9±2.3±3±4.2±4.3±4.5
>25to ≤32–±1.8±1.8±1.8±1.9±2.3±3±4.2±4.3±4.5
>32to ≤50–±1.8±1.8±1.8±1.9±2.3±3±4.2±4.3±4.5
>50to ≤100––±2.5±2.5±2.6±3±3.7±4.9±5.3±5.6
>100to ≤150––±3.2±3.3±3.4±3.7±4.4±5.7±6.1±6.4
>150to ≤200––±4±4±4.1±4.5±5.2±6.4±6.8±7.1
>200to ≤250–––––±5.2±5.9±7.2±7.6±7.9
>250to ≤300–––––±6±6.7±7.9±8.3±8.6