| Mechanical properties | Values |
|---|---|
| Young’s modulus | * 193 – 201 GPa |
| Specific stiffness | * 24.5 – 25.6 MN.m/kg |
| Yield strength (elastic limit) | 304 – 336 MPa |
| Tensile strength | 650 – 720 MPa |
| Specific strength | * 38.7 – 42.8 kN.m/kg |
| Elongation | 48.5 – 53.6 % strain |
| Compressive strength | * 304 – 336 MPa |
| Flexural modulus | * 193 – 201 GPa |
| Flexural strength (modulus of rupture) | * 304 – 336 MPa |
| Poisson’s ratio | * 0.265 – 0.275 |
| Shape factor | 58 |
| Hardness – Vickers | 180 – 208 HV |
| Hardness – Rockwell B | * 85 – 95 HRB |
| Hardness – Rockwell C | * 4 – 15 HRC |
| Hardness – Brinell | 217 – 245 HB |
| Elastic stored energy (springs) | * 684 – 1.4e3 kJ/m^3 |
| Fatigue strength at 10^7 cycles | * 293 – 323 MPa |
| Fatigue strength model (stress range) | * 275 – 344 MPa |
| *Values indicated with asterisks (*) are approximate. No guarantee is provided for the precision of this information. |