AISI 1141 Steel Overview

AISI 1141 steel (UNS G11410) is a resulfurized medium carbon steel. AISI 1141 is a free-machining grade: its raised sulfur content gives short chips and fast cutting speeds. This page lists the AISI 1141 material data sheets for 8 conditions: annealed, as rolled, normalized, oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 1141 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 1141 Steel Chemical Composition

C (carbon)0.37 – 0.45 %
Fe (iron)97.7 – 98.2 %
Mn (manganese)1.35 – 1.65 %
P (phosphorus)0 – 0.04 %
S (sulfur)0.08 – 0.13 %

AISI 1141 Steel Material Data Sheets

AISI 1141 Annealed Material Data Sheet

AISI 1141 As Rolled Material Data Sheet

AISI 1141 Normalized Material Data Sheet

AISI 1141 Oil Quenched & Tempered at 205°C Material Data Sheet

AISI 1141 Oil Quenched & Tempered at 315°C Material Data Sheet

AISI 1141 Oil Quenched & Tempered at 425°C Material Data Sheet

AISI 1141 Oil Quenched & Tempered at 540°C Material Data Sheet

AISI 1141 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 1141 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 1141 Annealed vs As Rolled vs Normalized vs Oil Quenched & Tempered (205–650°C): Yield, Tensile & Hardness Compared.

AISI 1141 Compared with Other Resulfurized Steels

Compare the composition, mechanical properties and machining speed of AISI 1141 with AISI 1117, 1118, 12L14, 1137, 1141 and 1144 in our resulfurized free-machining steels comparison.

AISI 1141 Steel Parts from Turkey

Looking for AISI 1141 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1141 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all medium and high carbon steel grades.