1.0737 Material Data Sheet: Non alloy quality steels

1.0737 Material Data Sheet: Non alloy quality steels: Steels with higher P or S content

Material Number1.0737
Steel groupNon alloy quality steels: Steels with higher P or S content
Symbol11SMnPb37; 9 SMnPb 36
StandardsDIN EN 10087 (01/1999) Free-cutting steels – Technical delivery conditions for semi-finished products, hot-rolled bars and rods.

DIN EN 10277-3 (06/2008) Bright steel products. Free-cutting steels. Steels not intended for heat treatment

Range of application: Free-cutting steels: Heavy duty free-cutting steel, with lead

1.0737 Material Composition

ElementMin/Max
C<=0.14
Si<=0.05
Mn1.00 – 1.50
P<=0.110
S0.340 – 0.400
Pb0.200 – 0.350
Key Additives: Mn + S + Pb

1.0737 Standard Comparison

CountrySymbolMaterial No.Standard
Australia12L14~1.07371442 (2007) (AU)
Australia12L14~1.07371443 (2004) (AU)
Austria11SMnPb371.0737EN 10087 (09/1998) (AT)
Austria11SMnPb371.0737EN 10277-3 (03/2008) (AT)
Belgium11SMnPb371.0737EN 10087 (09/1998) (BE)
Belgium11SMnPb371.0737EN 10277-3 (03/2008) (BE)
Bulgaria11SMnPb371.0737EN 10087 (09/1998) (BG)
Bulgaria11SMnPb371.0737EN 10277-3 (03/2008) (BG)
Cyprus11SMnPb371.0737EN 10087 (09/1998) (CY)
Cyprus11SMnPb371.0737EN 10277-3 (03/2008) (CY)
Czech Republic11SMnPb371.0737EN 10087 (09/1998) (CZ)
Czech Republic11SMnPb371.0737EN 10277-3 (03/2008) (CZ)
Denmark11SMnPb371.0737EN 10087 (09/1998) (DK)
Denmark11SMnPb371.0737EN 10277-3 (03/2008) (DK)
Estonia11SMnPb371.0737EN 10087 (09/1998) (EE)
Estonia11SMnPb371.0737EN 10277-3 (03/2008) (EE)
Europe11SMnPb371.073710087 (09/1998) (EUR)
Europe11SMnPb371.073710277-3 (03/2008) (EUR)
Finland11SMnPb371.0737EN 10087 (09/1998) (Fl)
Finland11SMnPb371.0737EN 10277-3 (03/2008) (Fl)
France11SMnPb371.0737EN 10087 (09/1998) (FR)
France11SMnPb371.0737EN 10277-3 (03/2008) (FR)
FranceS 300 Pb1.0737A 35-561 (1992) withdrawn (FR)
FranceS 300 Pb1.0737A 35-562 (1986) withdrawn (FR)
Great Britain11SMnPb371.0737EN 10087 (09/1998) (GB)
Great Britain11SMnPb371.0737EN 10277-3 (03/2008) (GB)
Greece11SMnPb371.0737EN 10087 (09/1998) (GR)
Greece11SMnPb371.0737EN 10277-3 (03/2008) (GR)
Hungary11SMnPb371.0737EN 10087 (09/1998) (HU)
Hungary11SMnPb371.0737EN 10277-3 (03/2008) (HU)
Iceland11SMnPb371.0737EN 10087 (09/1998) (IS)
Iceland11SMnPb371.0737EN 10277-3 (03/2008) (IS)
Ireland11SMnPb371.0737EN 10087 (09/1998) (IE)
Ireland11SMnPb371.0737EN 10277-3 (03/2008) (IE)
ISO12SMnPb35~(1.0737)683-9 (1988) (ISO)
Italy11SMnPb371.0737EN 10087 (09/1998) (IT)
Italy11SMnPb371.0737EN 10277-3 (03/2008) (IT)
ItalyCF 9 SMnPb 361.07374838 (1980) withdrawn (IT)
Latvia11SMnPb371.0737EN 10087 (09/1998) (LV)
Latvia11SMnPb371.0737EN 10277-3 (03/2008) (LV)
Lithuania11SMnPb371.0737EN 10087 (09/1998) (LT)
Lithuania11SMnPb371.0737EN 10277-3 (03/2008) (LT)
Luxemburg11SMnPb371.0737EN 10087 (09/1998) (LU)
Luxemburg11SMnPb371.0737EN 10277-3 (03/2008) (LU)
Malta11SMnPb371.0737EN 10087 (09/1998) (MT)
Malta11SMnPb371.0737EN 10277-3 (03/2008) (MT)
Netherlands11SMnPb371.0737EN 10087 (09/1998) (NL)
Netherlands11SMnPb371.0737EN 10277-3 (03/2008) (NL)
Norway11SMnPb371.0737EN 10087 (09/1998) (NO)
Norway11SMnPb371.0737EN 10277-3 (03/2008) (NO)
Poland11SMnPb371.0737EN 10087 (09/1998) (PL)
Poland11SMnPb371.0737EN 10277-3 (03/2008) (PL)
Portugal11SMnPb371.0737EN 10087 (09/1998) (PT)
Portugal11SMnPb371.0737EN 10277-3 (03/2008) (PT)
Romania11SMnPb371.0737EN 10087 (09/1998) (RO)
Romania11SMnPb371.0737EN 10277-3 (03/2008) (RO)
Serbia11SMnPb371.0737EN 10087 (09/1998) (CS)
Serbia11SMnPb371.0737EN 10277-3 (03/2008) (CS)
Slovak Republic11SMnPb371.0737EN 10087 (09/1998) (SK)
Slovak Republic11SMnPb371.0737EN 10277-3 (03/2008) (SK)
Slovenia11SMnPb371.0737EN 10087 (09/1998) (SL)
Slovenia11SMnPb371.0737EN 10277-3 (03/2008) (SL)
Spain11SMnPb371.0737EN 10087 (09/1998) (ES)
Spain11SMnPb371.0737EN 10277-3 (03/2008) (ES)
Spain12 SMnPb 351.073736021 (1980) withdrawn (ES)
SpainF.21141.073736021 (1980) withdrawn (ES)
Sweden11SMnPb371.0737EN 10087 (09/1998) (SE)
Sweden11SMnPb371.0737EN 10277-3 (03/2008) (SE)
Sweden1926~1.073714 1926withdrawn (SE)
Switzerland11SMnPb371.0737EN 10087 (09/1998) (CH)
Switzerland11SMnPb371.0737EN 10277-3 (03/2008) (CH)
Turkey11SMnPb371.0737EN 10087 (09/1998) (TR)
Turkey11SMnPb371.0737EN 10277-3 (03/2008) (TR)
U.S.A.G12144 (UNS)~1.0737
U.S.A.12L14 (AISI)~1.0737
U.S.A.A 29 (12L14) (ASTM)~1.0737A29-05(US)
U.S.A.A 108 (12L14) (ASTM)~1.0737A 108-07(US)
U.S.A.A 510 (12L14) (ASTM)~1.0737A 510-07/06(US)
U.S.A.A 519 (12L14) (ASTM)~1.0737A 519-06(US)
U.S.A.A 521(12L14) (ASTM)~1.0737A 521-06(US)
U.S.A.A 576 (12L14) (ASTM)~1.0737A 576-90 (06)(US)
U.S.A.A 711 (12L14) (ASTM)~1.0737A 711-07(US)
U.S.A.12L14 (SAE)~1.0737J 403 (2001) (US)

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey