AISI 4037 Low Alloy Steel

AISI 4037 Low Alloy Steel

AISI 4037 Steel Overview

AISI 4037 steel (UNS G40370) is a low alloy steel. This page lists the AISI 4037 material data sheets for 5 conditions: oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 4037 Steel

Heavy duty shafts, connecting rods, high tensile bolts

AISI 4037 Steel Chemical Composition

C (carbon)0.35 – 0.4 %
Fe (iron)98 – 98.6 %
Mn (manganese)0.7 – 0.9 %
Mo (molybdenum)0.2 – 0.3 %
P (phosphorus)0 – 0.035 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.35 %

AISI 4037 Steel Material Data Sheets

AISI 4037 Oil Quenched & Tempered at 205°C Material Data Sheet

AISI 4037 Oil Quenched & Tempered at 315°C Material Data Sheet

AISI 4037 Oil Quenched & Tempered at 425°C Material Data Sheet

AISI 4037 Oil Quenched & Tempered at 540°C Material Data Sheet

AISI 4037 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 4037 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 4037 Tempering Temperature Comparison (205–650°C): Yield, Tensile & Hardness.

AISI 4037 Steel Parts from Turkey

Looking for AISI 4037 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4037 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.