AISI 4130 Low Alloy Steel

AISI 4130 Low Alloy Steel

AISI 4130 Steel Overview

AISI 4130 steel (UNS G41300, EN 30CrMo4) is a low alloy steel. This page lists the AISI 4130 material data sheets for 8 conditions: annealed, air melted, normalized, air melted, quenched & tempered, water quenched & tempered at 205°C, water quenched & tempered at 315°C, water quenched & tempered at 425°C, water quenched & tempered at 540°C, water quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 4130 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 4130 Steel Chemical Composition

C (carbon)0.28 – 0.33 %
Cr (chromium)0.8 – 1.1 %
Fe (iron)97.3 – 98.2 %
Mn (manganese)0.4 – 0.6 %
Mo (molybdenum)0.15 – 0.25 %
P (phosphorus)0 – 0.035 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.35 %

AISI 4130 Steel Material Data Sheets

AISI 4130 Annealed Material Data Sheet

AISI 4130 Air Melted, Normalized Material Data Sheet

AISI 4130 Air Melted, Quenched & Tempered Material Data Sheet

AISI 4130 Water Quenched & Tempered at 205°C Material Data Sheet

AISI 4130 Water Quenched & Tempered at 315°C Material Data Sheet

AISI 4130 Water Quenched & Tempered at 425°C Material Data Sheet

AISI 4130 Water Quenched & Tempered at 540°C Material Data Sheet

AISI 4130 Water Quenched & Tempered at 650°C Material Data Sheet

AISI 4130 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 4130 Annealed vs Normalized vs Quenched & Tempered (205–650°C): Yield, Tensile & Hardness Compared.

AISI 4130 Steel Parts from Turkey

Looking for AISI 4130 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4130 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.