AISI 1022 steel (UNS G10220, EN 2C22) is a low carbon steel. This page lists the AISI 1022 material data sheets for 3 conditions: annealed, as rolled, normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.
Typical Uses of AISI 1022 Steel
General construction, general mechanical engineering, automotive, tools, axles, gears, springs.
Looking for AISI 1022 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1022 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low carbon steel grades.