| AISI 1141, Carbon steel Resulfurized, 0.41% C | Equivalent Grades |
|---|---|
| UNS number | G11410 |
| US name | ASTM G11410, ASTM 1141 Class B, ASTM 1141 Class A, ASTM 1141 |
| Italy name | 40SMnPb10 to UNI 4838 |
| France name | AFNOR NFA35562 45MF4 |
| JIS (Japanese) name | SUM42 to JIS G4804 |
Tradenames of AISI 1141, Carbon steel ( Resulfurized, 0.41% C ): AMERCUT C-1141, BETHLEHEM 33C, JALCASE 8, RY-AX, S-1141, STRAIN TEMPERED 1141
| Standards with similar compositions: |
|---|
| IAS IRAM 1141 (Argentina) |
| GB/T 15712(95) YF40MnV (China) |
| AFNOR NFA35562 45MF4 (France) |
| IS 1570 40Mn2S12 (India) |
| IS 5517 40Mn2S12 (India) |
| JIS G4804(83) SUM42 (Japan) |
| DGN B-296 1141 (Mexico) |
| NMX-B-301(86) 1141 (Mexico) |
| BS 970/1(83) 216A42 (United Kingdom) |
| ASTM A108(95) 1141 (USA) |
| ASTM A29/A29M(93) 1141 (USA) |
| ASTM A311/A311M(95) 1141 Class A (USA) |
| ASTM A311/A311M(95) 1141 Class B (USA) |
| ASTM A510(96) 1141 (USA) |
| ASTM A519(96) 1141 (USA) |
| ASTM A576(95) 1141 (USA) |
| FED QQ-S-633A(63) 1141 (USA) |
| FED QQ-S-637A(70) 1141 (USA) |
| SAE J1397(92) 1141 (USA) |
| SAE J403(95) 1141 (USA) |
| 1141 (USA) |
| AISI 1141 (USA) |
| COPANT 330 1141 (Venezuela) |
| COPANT 331 1141 (Venezuela) |
| COPANT 332 1141 (Venezuela) |
| COPANT 514 1141 (Venezuela) |
• Argentina:
IRAM 1141 to IAS
• India:
40C15S12 to IS 1570/3, 40C15S12 to IS 9175/13, 40Mn15S12 to IS 3930, 40Mn2S12 to IS 1570/3
• Italy:
40SMnPb10 to UNI 4838
• Japan:
SUM42 to JIS G4804
• Mexico:
1139 to NMX-B-301, 1141 to NMX-B-301
• Pan America:
1041 to COPANT 333, 1141 to COPANT 330, 1141 to COPANT 331, 1141 to COPANT 332, 1141 to COPANT 514
• USA:
1139, 1139 to ASTM A29/A29M, 1139 to SAE J1249, 1141, 1141 Class A to ASTM A311/A311M, 1141 Class B to ASTM A311/A311M, 1141 to ASTM A29/A29M, 1141 to ASTM A519, 1141 to FED QQ-S-633A, 1141 to FED QQ-S-637A, 1141 to SAE J403, C1139 to FED QQ-S-637A, G11390 to ASTM A510/A510M, G11390 to ASTM A576-90b, G11410 to ASTM A510/A510M, G11410 to ASTM A576-90b, UNS G11390, UNS G11410