1.0718 Material Data Sheet: Non alloy quality steels

1.0718 Material Data Sheet: Non alloy quality steels: Steels with higher P or S content

Material Number1.0718
Steel groupNon alloy quality steels: Steels with higher P or S content
Symbol11S11SMnPb30; 9 SMnPb 28
StandardsDIN EN 10087 (01/1999) Free-cutting steels – Technical delivery conditions for semi-finished products, hot-rolled bars and rods.

DIN EN 10277-3 (06/2008) Bright steel products. Free-cutting steels. Steels not intended for heat treatment

Range of application: Free-cutting steels: Heavy duty free-cutting steel, with lead

1.0718 Material Composition

ElementMin/Max
C<=0.14
Si<=0.05
Mn0.90 – 1.30
P<=0.110
S0.270 – 0.330
Pb0.200 – 0.350
Key Additives: Mn + S + Pb

1.0718 Standard Comparison

CountrySymbolMaterial No.Standard
Australia12L14~1.07181442 (2007) (AU)
Australia12L14~1.07181443 (2004) (AU)
Austria11SMnPb301.0718EN 10087 (09/1998) (AT)
Austria11SMnPb301.0718EN 10277-3 (03/2008) (AT)
Belgium11SMnPb301.0718EN 10087 (09/1998) (BE)
Belgium11SMnPb301.0718EN 10277-3 (03/2008) (BE)
Bulgaria11SMnPb301.0718EN 10087 (09/1998) (BG)
Bulgaria11SMnPb301.0718EN 10277-3 (03/2008) (BG)
BulgariaA9G-Rv1.07186886 (1974) withdrawn (BG)
Cyprus11SMnPb301.0718EN 10087 (09/1998) (CY)
Cyprus11SMnPb301.0718EN 10277-3 (03/2008) (CY)
Czech Republic11SMnPb301.0718EN 10087 (09/1998) (CZ)
Czech Republic11SMnPb301.0718EN 10277-3 (03/2008) (CZ)
Denmark11SMnPb301.0718EN 10087 (09/1998) (DK)
Denmark11SMnPb301.0718EN 10277-3 (03/2008) (DK)
Estonia11SMnPb301.0718EN 10087 (09/1998) (EE)
Estonia11SMnPb301.0718EN 10277-3 (03/2008) (EE)
Europe11SMnPb301.071810087 (09/1998) (EUR)
Europe11SMnPb301.071810277-3 (03/2008) (EUR)
Finland11SMnPb301.0718EN 10087 (09/1998) (Fl)
Finland11SMnPb301.0718EN 10277-3 (03/2008) (Fl)
France11SMnPb301.0718EN 10087 (09/1998) (FR)
France11SMnPb301.0718EN 10277-3 (03/2008) (FR)
FranceS 250 Pb1.0718A 35-561 (1992) withdrawn (FR)
FranceS 250 Pb1.0718A 35-562 (1986) withdrawn (FR)
Great Britain11SMnPb301.0718EN 10087 (09/1998) (GB)
Great Britain11SMnPb301.0718EN 10277-3 (03/2008) (GB)
Greece11SMnPb301.0718EN 10087 (09/1998) (GR)
Greece11SMnPb301.0718EN 10277-3 (03/2008) (GR)
Hungary11SMnPb301.0718EN 10087 (09/1998) (HU)
Hungary11SMnPb301.0718EN 10277-3 (03/2008) (HU)
Iceland11SMnPb301.0718EN 10087 (09/1998) (IS)
Iceland11SMnPb301.0718EN 10277-3 (03/2008) (IS)
Ireland11SMnPb301.0718EN 10087 (09/1998) (IE)
Ireland11SMnPb301.0718EN 10277-3 (03/2008) (IE)
ISO11SMnPb28~(1.0718)683-9 (1988) (ISO)
Italy11SMnPb301.0718EN 10087 (09/1998) (IT)
Italy11SMnPb301.0718EN 10277-3 (03/2008) (IT)
ItalyCF 9 SMnPb 281.07184838 (1980) withdrawn (IT)
JapanSUM 22 L~1.0718G 4804 (2008) (JP)
JapanSUM 23 L~1.0718G 4804 (2008) (JP)
JapanSUM 24 L~1.0718G 4804 (2008) (JP)
Latvia11SMnPb301.0718EN 10087 (09/1998) (LV)
Latvia11SMnPb301.0718EN 10277-3 (03/2008) (LV)
Lithuania11SMnPb301.0718EN 10087 (09/1998) (LT)
Lithuania11SMnPb301.0718EN 10277-3 (03/2008) (LT)
Luxemburg11SMnPb301.0718EN 10087 (09/1998) (LU)
Luxemburg11SMnPb301.0718EN 10277-3 (03/2008) (LU)
Malta11SMnPb301.0718EN 10087 (09/1998) (MT)
Malta11SMnPb301.0718EN 10277-3 (03/2008) (MT)
Netherlands11SMnPb301.0718EN 10087 (09/1998) (NL)
Netherlands11SMnPb301.0718EN 10277-3 (03/2008) (NL)
Norway11SMnPb301.0718EN 10087 (09/1998) (NO)
Norway11SMnPb301.0718EN 10277-3 (03/2008) (NO)
Poland11SMnPb301.0718EN 10087 (09/1998) (PL)
Poland11SMnPb301.0718EN 10277-3 (03/2008) (PL)
Portugal11SMnPb301.0718EN 10087 (09/1998) (PT)
Portugal11SMnPb301.0718EN 10277-3 (03/2008) (PT)
Republc of KoreaSUM 22L~1.0718D 3567 (2002) (KR)
Republc of KoreaSUM 23L~1.0718D 3567 (2002) (KR)
Republc of KoreaSUM 24L~1.0718D 3567 (2002) (KR)
Romania11SMnPb301.0718EN 10087 (09/1998) (RO)
Romania11SMnPb301.0718EN 10277-3 (03/2008) (RO)
Serbia11SMnPb301.0718EN 10087 (09/1998) (CS)
Serbia11SMnPb301.0718EN 10277-3 (03/2008) (CS)
SerbiaC3993 t1.0718C.B0.505 (1984) withdrawn (CS)
Slovak Republic11SMnPb301.0718EN 10087 (09/1998) (SK)
Slovak Republic11SMnPb301.0718EN 10277-3 (03/2008) (SK)
Slovenia11SMnPb301.0718EN 10087 (09/1998) (SL)
Slovenia11SMnPb301.0718EN 10277-3 (03/2008) (SL)
Spain11SMnPb301.0718EN 10087 (09/1998) (ES)
Spain11SMnPb301.0718EN 10277-3 (03/2008) (ES)
SpainF.210.C~1.0718Non standardized steels (ES)
SpainF.210.M~1.0718Non standardized steels (ES)
Spain11SMnPb 28 t1.071836021 (1980) withdrawn (ES)
SpainF.21121.071836021 (1980) withdrawn (ES)
Sweden11SMnPb301.0718EN 10087 (09/1998) (SE)
Sweden11SMnPb301.0718EN 10277-3 (03/2008) (SE)
Sweden1914~1.071814 1914withdrawn (SE)
Switzerland11SMnPb301.0718EN 10087 (09/1998) (CH)
Switzerland11SMnPb301.0718EN 10277-3 (03/2008) (CH)
Turkey11SMnPb301.0718EN 10087 (09/1998) (TR)
Turkey11SMnPb301.0718EN 10277-3 (03/2008) (TR)
U.S.A.G12134 (UNS)~1.0718
U.S.A.G12144 (UNS)~1.0718
U.S.A.12L14 (AISI)~1.0718
U.S.A.12L13 (AISI)~1.0718
U.S.A.A 29 (12L13) (ASTM)~1.0718A29-05(US)
U.S.A.A 29 (12L14) (ASTM)~1.0718A29-05(US)
U.S.A.A 108 (12L13) (ASTM)~1.0718A 108-07(US)
U.S.A.A 108 (12L14) (ASTM)~1.0718A 108-07(US)
U.S.A.A 510 (12L13) (ASTM)~1.0718A 510-07/06(US)
U.S.A.A 510 (12L14) (ASTM)~1.0718A 510-07/06(US)
U.S.A.A 519 (12L14) (ASTM)~1.0718A 519-06(US)
U.S.A.A 521 (12L14) (ASTM)~1.0718A 521-06(US)
U.S.A.A 521 (12L13) (ASTM)~1.0718A 521-06(US)
U.S.A.A 576 (12L14) (ASTM)~1.0718A 576-90 (06)(US)
U.S.A.A 711 (12L13) (ASTM)~1.0718A 711-07(US)
U.S.A.A 711 (12L14) (ASTM)~1.0718A 711-07(US)
U.S.A.12L14 (SAE)~1.0718J 403 (2001) (US)
U.S.A.12L13 (SAE)~1.0718Non standardized steels (US)

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey