AM-355 SCT 1000 Stainless Steel Material Data Sheet (Semi-austenitic, Precipitation Hardened)
AM-355 SCT 1000 Stainless Steel Overview
AM-355 SCT 1000 stainless steel is a semi-austenitic precipitation hardening stainless steel (UNS S35500) in the wrought form. Condition: SCT 1000 (Solution annealed; hardened by sub-zero cooling and tempering 540°C). This AM-355 SCT 1000 stainless steel material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for AM-355 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AM-355 parts in-house and inspects them before shipment.
AM-355 Designation
AM-355, wrought Condition SCT 1000 (Solution annealed; hardened by sub-zero cooling and tempering 540°C) UNS number S35500 US name AM-355
AM-355 Typical uses
Processing of potentially corrosive liquids e.g. chemicals/oil/beverages/sewage, structural uses in corrosive environments, e.g. nuclear plants, ships, offshore oil installations, underwater cables and pipes
AM-355 SCT 1000 Stainless Steel Composition detail
C (carbon) 0.1 – 0.15 % Cr (chromium) 15 – 16 % Fe (iron) 73.6 – 77.8 % Mn (manganese) 0.5 – 1.25 % Mo (molybdenum) 2.5 – 3.25 % N (nitrogen) 0.07 – 0.13 % Ni (nickel) 4 – 5 % P (phosphorus) 0 – 0.04 % S (sulfur) 0 – 0.03 % Si (silicon) 0 – 0.5 %
AM-355 Physical properties
AM-355 SCT 1000 Stainless Steel Mechanical properties
Young’s modulus 200 – 210 GPa Specific stiffness 25.6 – 26.9 MN.m/kg Yield strength (elastic limit) 1070 – 1180 MPa Tensile strength 1170 – 1300 MPa Specific strength 137 – 151 kN.m/kg Elongation 12 – 13.9 % strain Compressive strength 1100 – 1220 MPa Flexural modulus 200 – 210 GPa Flexural strength (modulus of rupture) 1070 – 1180 MPa Shear modulus 76 – 79.9 GPa Bulk modulus 185 – 195 GPa Poisson’s ratio 0.32 – 0.333 Shape factor 21 Hardness – Vickers 350 – 380 HV Hardness – Rockwell B 110 – 113 HRB Hardness – Rockwell C 37 – 43 HRC Hardness – Brinell 352 – 390 HB Elastic stored energy (springs) 2790 – 3410 kJ/m3 Fatigue strength at 10^7 cycles 469 – 527 MPa Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles 444 – 557 MPa
AM-355 Impact & fracture properties
Fracture toughness 104 – 127 MPa.m0.5 Toughness (G) 52.7 – 77.4 kJ/m2
AM-355 SCT 1000 Stainless Steel Thermal properties
Melting point 1400 – 1440 °C Maximum service temperature 382 – 427 °C Minimum service temperature -73 – -43 °C Thermal conductivity 15.6 – 16.9 W/m.°C Specific heat capacity 490 – 510 J/kg.°C Thermal expansion coefficient 12.1 – 12.7 µstrain/°C Thermal shock resistance 417 – 471 °C Thermal distortion resistance 1.25 – 1.38 MW/m Latent heat of fusion 308 – 379 kJ/kg
AM-355 Electrical properties
Electrical resistivity 75.3 – 104 µohm.cm Electrical conductivity 1.65 – 2.29 %IACS Galvanic potential -0.21 – -0.13 V
AM-355 Magnetic properties
AM-355 Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 5060 – 5190 m/s Mechanical loss coefficient (tan delta) 3.1e-4 – 6.6e-4
AM-355 Processing properties
Metal casting Unsuitable Metal cold forming Limited use Metal hot forming Acceptable Metal press forming Acceptable Metal deep drawing Unsuitable Machining speed 11.3 m/min Weldability Notes: Preheating is not required, post weld heat treatment is required Good Weldability – MIG Good Weldability – plasma Good Weldability – SAW Not recommended Weldability – TIG Good Brazeability Good Carbon equivalency 3.95 – 4.54
AM-355 Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Acceptable Weak alkalis Excellent Strong alkalis Limited use Organic solvents Excellent Oxidation at 500C Excellent UV radiation (sunlight) Excellent Galling resistance (adhesive wear) Notes: Aluminum bronze is the most suitable mating material to minimize galling. Limited use Flammability Non-flammable
AM-355 SCT 1000 Stainless Steel Corrosion resistance
Pitting resistance equivalent number (PREN) 24.4 – 28.8 Pitting and crevice corrosion Medium (20-30) Stress corrosion cracking Note: Rated in chloride; Other susceptible environments: Hydrogen sulfide Susceptible Intergranular (weld line) corrosion Good Inorganic acids Restricted Organic acids Moderate Alkalis Moderate Humidity / water Excellent Sea water Restricted Sour oil and gas Restricted
AM-355 Notes
AM-355 SCT 1000 Warning Check with supplier what tempering and aging procedure has been applied – it could make a major difference to the steel’s mechanical properties.
AM-355 Standards with similar compositions
USA: 5549 to AMS 5549F, 64 to ASTM A579, AM-355 to SAE J467, S35500 to ASTM A564/A564M, S35500 to ASTM A705/A705M-95, UNS S35500, UNS S35580Tradenames: AM 355, AM-355, CRONIFER 1505 MON – ALLOY 355, SLATER AM355, UNITEMP 355