AISI 1340 steel (UNS G13400, EN 38Mn6) is a medium carbon manganese steel. In the SAE numbering system the 13xx series is classed as a manganese alloy steel; it contains about 1.6–1.9% manganese, well above plain carbon steel. This page lists the AISI 1340 material data sheets for 7 conditions: annealed, normalized, oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.
Typical Uses of AISI 1340 Steel
General construction, general mechanical engineering, automotive, tools, axles, gears, springs.
Looking for AISI 1340 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1340 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all medium and high carbon steel grades.