| Mechanical properties | Values |
|---|---|
| Young’s modulus | * 190 – 210 GPa |
| Specific stiffness | * 24.3 – 27 MN.m/kg |
| Yield strength (elastic limit) | 310 – 340 MPa |
| Tensile strength | 612 – 880 MPa |
| Specific strength | * 39.7 – 43.7 kN.m/kg |
| Elongation | 40 – 50 % strain |
| Compressive strength | * 275 – 515 MPa |
| Flexural modulus | * 190 – 210 GPa |
| Flexural strength (modulus of rupture) | 275 – 515 MPa |
| Shear modulus | * 74 – 84 GPa |
| Bulk modulus | * 134 – 156 GPa |
| Poisson’s ratio | 0.265 – 0.275 |
| Shape factor | 58 |
| Hardness – Vickers | * 192 – 250 HV |
| Hardness – Rockwell B | 85 – 95 HRB |
| Hardness – Rockwell C | * 9 – 23 HRC |
| Hardness – Brinell | 228 – 254 HB |
| Elastic stored energy (springs) | * 463 – 693 kJ/m^3 |
| Fatigue strength at 10^7 cycles | * 268 – 386 MPa |
| Fatigue strength model (stress range) | * 222 – 466 MPa |
| *Values indicated with asterisks (*) are approximate. No guarantee is provided for the precision of this information. |