Thermal Welding

mig welding_modulus metal

Welcome to the Modulus Metal Welding Services page! We offer a variety of high-quality welding services to meet your manufacturing needs. Below, you will find explanations of each welding process we offer.

  • Arc Spot – MIG
  • Arc Spot – TIG
  • Brazing
  • Gas Metal Arc (MIG)
  • Gas Tungsten Arc (TIG)
  • Manual Metal Arc (MMA)
  • Oxyacetylene
  • Soldering
  • Submerged Arc
  • Thermit Welding

Arc Spot – MIG: Arc spot MIG welding is a process in which an electric arc is used to weld two or more metal pieces together using a wire electrode and an inert gas. This process is often used to create small, precise welds, and is particularly well-suited for use in automated welding systems.

Arc Spot – TIG: Arc spot TIG welding is a process in which an electric arc is used to weld two or more metal pieces together using a tungsten electrode and an inert gas. This process is often used to create small, precise welds, and is particularly well-suited for use in automated welding systems.

Brazing: Brazing is a process in which two or more metal pieces are joined together using a filler metal with a melting temperature above 450°C. This process is often used to create strong, reliable joints, and is particularly well-suited for use in high-temperature applications.

Gas Metal Arc (MIG): Gas metal arc (MIG) welding is a process in which an electric arc is used to weld two or more metal pieces together using a wire electrode and an inert gas. This process is often used to create strong, reliable welds, and is particularly well-suited for use in automated welding systems.

Gas Tungsten Arc (TIG): Gas tungsten arc (TIG) welding is a process in which an electric arc is used to weld two or more metal pieces together using a tungsten electrode and an inert gas. This process is often used to create high-quality welds, and is particularly well-suited for use on thin materials or for creating precise welds.

Manual Metal Arc (MMA): Manual metal arc (MMA) welding is a process in which an electric arc is used to weld two or more metal pieces together using a consumable electrode. This process is often used to create strong, reliable welds, and is particularly well-suited for use in outdoor or field applications.

Oxyacetylene: Oxyacetylene welding is a process in which two or more metal pieces are joined together using a flame produced by the combustion of acetylene and oxygen. This process is often used to create strong, reliable welds, and is particularly well-suited for use in field or repair applications.

Soldering: Soldering is a process in which two or more metal pieces are joined together using a filler metal with a melting temperature below 450°C. This process is often used to create electrical or mechanical connections and is particularly well-suited for use on thin materials or in applications where the joint is not subject to high stresses.

Submerged Arc: Submerged arc welding is a process in which an electric arc is used to weld two or more metal pieces together using a consumable electrode. This process is often used to create strong, reliable welds, and is particularly well-suited for use in high-production welding operations.

Thermit Welding: Thermit welding is a process in which two or more metal pieces are joined together using a thermit reaction, in which a thermite mixture is ignited to produce extremely high temperatures. This process is often used to create strong, reliable welds, and is particularly well-suited for use in field or repair applications.

We hope this information has been helpful in understanding the welding services we offer at Modulus Metal Company. Thank you for considering us for your manufacturing needs.

ISO 13920 Welding Tolerance Calculator by Modulus Metal Turkey
welding_modulus metal
Valve Welding_Modulus Metal

USEFUL INFO

List of Welding Codes


American Society of Mechanical Engineers (ASME) Codes


The American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (BPVC) covers all aspects of design and manufacture of boilers and pressure vessels. All sections contain welding specifications, however most relevant information is contained in the following:


Code Description


ASME BPVC Section II Part C: Specifications for Welding Rods, Electrodes, and Filler Metals.[1]

ASME BPVC Section V Nondestructive Examination
ASME BPVC Section IX Welding and Brazing Qualifications

ASME B16.25 Buttwelding ends magi

American Welding Society (AWS) Standards


The American Welding Society (AWS) publishes over 240 AWS-developed codes, recommended practices and guides which are written in accordance with American National Standards Institute (ANSI) practices.[2] The following is a partial list of the more common publications:


Standard Number† Title


AWS A02.4 Standard symbols for welding, brazing, and non-destructive examination
AWS A03.0 Standard welding terms and definitions
AWS A05.1 Specification for carbon steel electrodes for shielded metal arc welding
AWS A05.18 Specification for carbon steel electrodes and rots for gas shielded arc welding
AWS B01.10 Guide for the nondestructive examination of welds
AWS B02.1 Specification for Welding Procedure and Performance Qualification
AWS D01.1 Structural welding (steel)
AWS D01.2 Structural welding (aluminum)
AWS D01.3 Structural welding (sheet steel)
AWS D01.4 Structural welding (reinforcing steel)
AWS D01.5 Bridge welding
AWS D01.6 Structural welding (stainless steel)
AWS D01.7 Structural welding (strengthening and repair)
AWS D01.8 Structural welding seismic supplement
AWS D01.9 Structural welding (titanium)
AWS D08.1 Automotive spot welding
AWS D08.6 Automotive spot welding electrodes supplement
AWS D08.7 Automotive spot welding recommendations supplement
AWS D08.8 Automotive arc welding (steel)
AWS D08.9 Automotive spot weld testing
AWS D08.14 Automotive arc welding (aluminum)
AWS D09.1 Sheet metal welding
AWS D10.10 Heating practices for pipe and tube
AWS D10.11 Root pass welding for pipe
AWS D10.12 Pipe welding (mild steel)
AWS D10.13 Tube brazing (copper)
AWS D10.18 Pipe welding (stainless steel)
AWS D11.2 Welding (cast iron)
AWS D14.1 Industrial mill crane welding
AWS D14.3 Earthmoving & agricultural equipment welding
AWS D14.4 Machinery joint welding
AWS D14.5 Press welding
AWS D14.6 Industrial mill roll surfacing
AWS D15.1 Railroad welding
AWS D15.2 Railroad welding practice supplement
AWS D16.1 Robotic arc welding safety
AWS D16.2 Robotic arc welding system installation
AWS D16.3 Robotic arc welding risk assessment
AWS D16.4 Robotic arc welder operator qualification
AWS D17.1 Aerospace fusion welding
AWS D17.2 Aerospace resistance welding
AWS D18.1 Hygienic tube welding (stainless steel)
AWS D18.2 Stainless steel tube discoloration guide
AWS D18.3 Hygienic equipment welding
†The zero after the first letter is only placed there so the table can be sorted. i.e. D01.1 is actually D1.1).

American Petroleum Institute (API) Standards
The American Petroleum Institute (API) oldest and most successful programs is in the development of API standards which started with its first standard in 1924. API maintains over 500 standards covering the oil and gas field.[3] The following is a partial list specific to welding:


Standard Number Description


API RP 577 Welding Inspection and Metallurgy
API 1104 Welding of pipelines and related facilities


Australian / New Zealand (AS/NZS) Standards


Standards Australia is the body responsible for the development, maintenance and publication of Australian Standards.[4] The following is a partial list specific to welding:


Standard Number Description


AS/NZS 1554.1 Structural steel welding – Welding of steel structures
AS/NZS 1554.2 Structural steel welding – Stud welding (steel studs to steel)
AS/NZS 1554.3 Structural steel welding – Welding of reinforcing steel
AS/NZS 1554.4 Structural steel welding – Welding of high strength quenched and tempered steels
AS/NZS 1554.5 Structural steel welding – Welding of steel structures subject to high levels of fatigue loading
AS/NZS 1554.6 Structural steel welding – Welding stainless steels for structural purposes
AS/NZS 1554.7 Structural steel welding – Welding of sheet steel structures
AS/NZS 3992 Pressure equipment – Welding and brazing qualification

Canadian Standards Association (CSA) Standards


The Canadian Standards Association (CSA) is responsible for the development, maintenance and publication of CSA standards.[5] The following is a partial list specific to welding:


Standard Number Description


CAN/CSA-G401-07 Corrugated Steel Pipe Products
CAN/CSA-ISO 14341:11 Welding consumables – Wire electrodes and weld deposits for gas shielded metal arc welding of non alloy and fine grain steels –

CAN/CSA-W117.2-06 (R2011) Safety in Welding, Cutting and Allied Processes
G40.20-04/G40.21-04 (R2009) General Requirements for Rolled or Welded Structural Quality Steel/ Structural Quality Steel
W178.1-08 Certification of Welding Inspection Organizations
W178.2-08 Certification of Welding Inspectors
W47.1-09 Certification of companies for fusion welding of steel
W47.2-11 Certification of companies for fusion welding of aluminum
W48-06 (R2011) Filler Metals and Allied Materials for Metal Arc Welding
W55.3-08 Certification of companies for resistance welding of steel and aluminum
W59-13 Welded Steel Construction (Metal Arc Welding)
W59.2-M1991 (R2008) Welded Aluminum Construction
Z662-11 Oil and Gas Pipeline Systems


British Standards (BS)


British Standards are developed, maintained and published by BSI Standards which is UK’s National Standards Body.[6] The following is a partial list of standards specific to welding:

Standard Number Description


BS 499-1 Welding terms and symbols. Glossary for welding, brazing and thermal cutting
BS 499-2C Welding terms and symbols. European arc welding symbols in chart form
BS 2633 Specification for Class I arc welding of ferritic steel pipework for carrying fluids
BS 2971 Specification for class II arc welding of carbon steel pipework for carrying fluids
BS 4515-1 Specification for welding of steel pipelines on land and offshore – Part 1: Carbon and carbon manganese steel pipelines
BS 4515-2 Specification for welding of steel pipelines on land and offshore. Duplex stainless steel pipelines
PD 6705-2 Structural use of steel and aluminium. Recommendations for the execution of steel bridges to BS EN 1090-2
PD 6705-3 Structural use of steel and aluminium. Recommendations for the execution of
aluminium structures to BS EN 1090-3

International Organization for Standardization (ISO) Standards


International Organization for Standardization (ISO) has developed over 18500 standards and over 1100 new standards are published every year.[7] The following is a partial list of the standards specific to welding:


Standard Number Description


ISO 2553 Welded, brazed and soldered joints – symbolic representation on drawings (1992)
ISO 2560 Welding consumables. Covered electrodes for manual metal arc welding of non-alloy and fine grain steels. Classification
ISO 3580 Covered electrodes for manual arc welding of creep-resisting steels – Code of symbols for identification
ISO 3581 Covered electrodes for manual arc welding of stainless and other similar high alloy steels – Code of symbols for identification
ISO 3834 Quality requirements for fusion welding of metallic materials, five parts.
ISO 4063 Welding and allied processes – Nomenclature of processes and reference numbers
ISO 5817 Welding. Fusion-welded joints in steel, nickel, titanium and their alloys (beam welding excluded). Quality levels for imperfections
ISO 6520-1 Welding and allied processes — Classification of geometric imperfections in metallic materials — Part 1: Fusion welding
ISO 6520-2 Welding and allied processes — Classification of geometric imperfections in metallic materials — Part 2: Welding with pressure
ISO 6947 Welds. Working positions. Definitions of angles of slope and rotation
ISO 9606 Qualification test of welders — Fusion welding, parts 1 to 5
ISO 9692-1 Welding and allied processes. Recommendations for joint preparation. Manual metal-arc welding, gas-shielded metal-arc welding, gas welding, TIG welding and beam welding of steels
ISO 9692-2 Welding and allied processes. Joint preparation. Submerged arc welding of steels
ISO 9692-3 Welding and allied processes. Joint preparation. Part 3: TIG and MIG welding of
aluminium and its alloys
ISO 13847 Petroleum and natural gas industries – Pipeline transportation systems – Welding of pipelines
ISO 13916 Welding – Guidance on the measurement of preheating temperature, interpass temperature and preheat maintenance temperature
ISO 13918 Welding – Studs and ceramic ferrules for arc stud welding
ISO 13919-1 Welding – Electron and laser-beam welded joints – Guidance on quality level for
imperfections – Part 1: Steel
ISO 13919-2 Welding – Electron and laser-beam welded joints – Guidance on quality level for
imperfections – Part 2: Aluminium and its weldable alloys
ISO 13920 Welding – General tolerances for welded constructions – Dimensions for lengths and angles Shape and position
ISO 14112 Gas welding equipment – Small kits for gas brazing and welding
ISO 14175 Welding consumables — Gases and gas mixtures for fusion welding and allied processes.Replaced EN 439:1994 in Europe.
ISO 14341 Welding consumables. Wire electrodes and deposits for gas shielded metal arc welding of non alloy and fine grain steels. Classification
ISO 14554 Resistance welding

ISO 14744 Electron beam welding, six parts

ISO 15607 Specification and qualification of welding procedures for metallic materials – General rules

ISO/TR 15608 Welding – Guidelines for a metallic material grouping system

ISO 15609 Specification and qualification of welding procedures for metallic materials – Welding procedure specification, five parts.

ISO 15610 Specification and qualification of welding procedures for metallic materials-Qualification based on tested welding consumables

ISO 15611 Specification and qualification of welding procedures for metallic materials —Qualification based on previous welding experience

ISO 15612 Specification and qualification of welding procedures for metallic materials —Qualification by adoption of a standard welding procedure

ISO 15613 Specification and qualification of welding procedures for metallic materials —

Qualification based on pre-production welding test

ISO 15614 Specification and qualification of welding procedures for metallic materials – Welding procedure test, 13 parts.

ISO 15615 Gas welding equipment. Acetylene manifold systems for welding, cutting and allied processes. Safety requirements in high-pressure devices

ISO 15618-1 Qualification testing of welders for under-water welding. Diver-welders for hyperbaric wet welding

ISO 15618-2 Qualification testing of welders for under-water welding. Diver-welders and welding operators for hyperbaric dry welding

ISO 17635 Non-destructive testing of welds. General rules for metallic materials

ISO/TR 20172 Welding — Grouping systems for materials — European materials

ISO/TR 20173 Welding — Grouping systems for materials — American materials

ISO/TR 20174 Welding — Grouping systems for materials — Japanese materials

ISO 24394 Welding for aerospace applications. Qualification test for welders and welding operators.Fusion welding of metallic components

European Union (CEN) standards

The European Committee for Standardization (CEN) had issued numerous standards covering welding processes, which unified and replaced former national standards. Of the former national standards, those issued by BSI and DIN were widely used outside their countries of origin. After the Vienna Agreement with ISO, CEN has replaced most of them with equivalent ISO standards (EN ISO series).[8]

Standard Number Description

EN 287-1 Qualification test of welders — Fusion welding — Part 1: Steels[9] [10]

EN 1090-1 Execution of steel structures and aluminium structures – Part 1: Requirements for conformity assessment of structural components

EN 1090-2 Execution of steel structures and aluminium structures – Part 2: Technical requirements for steel structures

EN 1090-3 Execution of steel structures and aluminium structures – Part 3: Technical requirements for aluminium structures

EN 1011-1 Welding — Recommendations for welding of metallic materials — Part 1: General
guidance for arc welding
EN 1011-2 Welding — Recommendations for welding of metallic materials — Part 2: Arc welding of ferritic steels
EN 1011-3 Welding — Recommendations for welding of metallic materials — Part 3: Arc welding of stainless steels
EN 1011-4 Welding — Recommendations for welding of metallic materials — Part 4: Arc welding of aluminium and aluminium alloys
EN 1011-5 Welding. Recommendations for welding of metallic materials. Welding of clad steel
EN 1011-6 Welding. Recommendations for welding of metallic materials. Laser beam welding
EN 1011-7 Welding — Recommendations for welding of metallic materials — Part 7: Electron beam welding
EN 1011-8 Welding. Recommendations for welding of metallic materials. Welding of cast irons
EN 1418 Welding personnel. Approval testing of welding operators for fusion welding and
resistance weld setters for fully mechanized and automatic welding of metallic materials
EN 1708-1 Welding. Basic welded joint details in steel. Pressurized components.
EN 1708-2 Welding. Basic weld joint details in steel. Non-internal pressurized components.
EN 1708-3 Welding. Basic weld joint details in steel. Clad, buttered and lined pressurized
components.
EN 1993-1-8 Eurocode 3: Design of steel structures – Part 1-8: General – Design of joints
EN 13133 Brazing – Brazer approval
EN 22553 Welded, brazed and soldered joints – Symbolic representation on drawings. (CEN version of ISO 2553)


Additional requirements for welding exist in CEN codes and standards for specific products, like EN12952, EN 12953, EN 13445, EN 13480, etc.


German Standards (DIN and others)


NA 092 is the Standards Committee for welding and allied processes (NAS) at DIN Deutsches Institut für Normung e. V.[11] The following is a partial list of DIN welding standards:


Code Description


DIN 1910-100 Welding; terms dependent on materials for metal welding
SEW 088 Schweißgeeignete Feinkornbaustähle – Richtlinien für die Verarbeitung besonders für
das Schmelzschweißen”, Stahlinstitut VDEh

Merkblatt DVS 0916 Metall-Schutzgasschwißen von Feinkornbaustählen”, Deutsche Verband für Schweißtechnik e.V.