Low alloy steels are carbon steels with small, deliberate additions of chromium, molybdenum, nickel, vanadium, silicon or boron, usually totalling less than about 5%. These additions raise hardenability, strength and toughness compared with plain carbon steel, so parts can be through-hardened by quenching and tempering in larger sections. Low alloy steels are the workhorse materials for shafts, gears, axles, bolts, crankshafts, springs and high-strength structural and aerospace components.
AISI and SAE Low Alloy Steel Numbering
In the AISI/SAE four-digit system the first two digits identify the main alloying elements and the last two give the nominal carbon content in hundredths of a percent. For example, 41xx steels are chromium-molybdenum steels and AISI 4140 contains about 0.40% carbon; 43xx and 86xx are nickel-chromium-molybdenum steels, 51xx are chromium steels and 92xx are silicon-manganese spring steels. A letter B in the middle, as in 50B46 or 94B30, shows that a small boron addition is used to increase hardenability.
Low Alloy Steel Heat Treatment Conditions
The same low alloy steel can have very different properties depending on its heat treatment. Annealed material is softest and easiest to machine. Normalizing gives a finer, more uniform structure with higher strength. Quenching and tempering produces the highest strength: tempering at a low temperature such as 205°C keeps hardness and tensile strength very high, while tempering at 540–650°C lowers strength but greatly improves toughness and ductility. Each grade below has separate data sheets for each condition, and a comparison post shows how yield strength, tensile strength and hardness change between them.
Low Alloy Steel Parts from Turkey
Looking for low alloy steel parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined low alloy steel parts in-house, including AISI 4140, 4340 and 8620, supplies them heat treated to the required condition, and inspects them before shipment.