1.0715 Material Data Sheet: Non alloy quality steels

1.0715 Material Data Sheet: Non alloy quality steels: Steels with higher P or S content

Material Number1.0715
Steel groupNon alloy quality steels: Steels with higher P or S content
Symbol11SMn30; 9 SMn 28
StandardsDIN EN 10087 (01/1999) Free-cutting steels – Technical delivery conditions for semi-finished products, hot-rolled bars and rods.

DIN EN 10277-3 (06/2008) Bright steel products. Free-cutting steels. Steels not intended for heat treatment

Range of application: Free-cutting steels: Heavy duty free-cutting steel

1.0715 Material Composition

ElementMin/Max
C <=0.14
Si<=0.05
Mn0.90 – 1.30
P<=0.110
S0.270 – 0.330
Key Additives: Mn + S

1.0715 Standard Comparison

CountrySymbolMaterial NoStandard
Australia1214~1.07151442 (2007) (AU)
AustraliaS1214~1.07151448 (2007) (AU)
Austria11SMn301.0715EN 10087 (09/1998) (AT)
Austria11SMn301.0715EN 10277-3 (03/2008) (AT)
Belgium11SMn301.0715EN 10087 (09/1998) (BE)
Belgium11SMn301.0715EN 10277-3 (03/2008) (BE)
Bulgaria11SMn301.0715EN 10087 (09/1998) (BG)
Bulgaria11SMn301.0715EN 10277-3 (03/2008) (BG)
Cyprus11SMn301.0715EN 10087 (09/1998) (CY)
Cyprus11SMn301.0715EN 10277-3 (03/2008) (CY)
Czech Republic11109~1.0715411109 (1974) (CZ)
Czech Republic11SMn301.0715EN 10087 (09/1998) (CZ)
Czech Republic11SMn301.0715EN 10277-3 (03/2008) (CZ)
Denmark11SMn301.0715EN 10087 (09/1998) (DK)
Denmark11SMn301.0715EN 10277-3 (03/2008) (DK)
Estonia11SMn301.0715EN 10087 (09/1998) (EE)
Estonia11SMn301.0715EN 10277-3 (03/2008) (EE)
Europe11SMn301.071510087 (09/1998) (EUR)
Europe11SMn301.071510277-3 (03/2008) (EUR)
Finland11SMn301.0715EN 10087 (09/1998) (Fl)
Finland11SMn301.0715EN 10277-3 (03/2008) (Fl)
France11SMn301.0715EN 10087 (09/1998) (FR)
France11SMn301.0715EN 10277-3 (03/2008) (FR)
Frances 2501.0715A 35-561 (1992) withdrawn (FR)
Frances 2501.0715A 35-562 (1986) withdrawn (FR)
Great Britain11SMn301.0715EN 10087 (09/1998) (GB)
Great Britain11SMn301.0715EN 10277-3 (03/2008) (GB)
Great Britain230 M 071.0715970 Part 1(1996) withdrawn (GB)
Great Britain230 M 071.0715970 Part 3 (1991) withdrawn (GB)
Greece11SMn301.0715EN 10087 (09/1998) (GR)
Greece11SMn301.0715EN 10277-3 (03/2008) (GR)
Hungary11SMn301.0715EN 10087 (09/1998) (HU)
Hungary11SMn301.0715EN 10277-3 (03/2008) (HU)
Iceland11SMn301.0715EN 10087 (09/1998) (IS)
Iceland11SMn301.0715EN 10277-3 (03/2008) (IS)
India11C10S25~1.07151570 Part Ill (1979) (IN)
India11S25 t~1.07151570 Part Ill (1979) (IN)
India11C10S25~1.07154431 (1978) (IN)
India11C10S25~1.07154432 (1988) (IN)
Ireland11SMn301.0715EN 10087 (09/1998) (IE)
Ireland11SMn301.0715EN 10277-3 (03/2008) (IE)
ISO11SMn28~(1.0715)683-9 (1988) (ISO)
Italy11SMn301.0715EN 10087 (09/1998) (IT)
Italy11SMn301.0715EN 10277-3 (03/2008) (IT)
ItalyCF 9 S 221.07154838 (1980) withdrawn (IT)
JapanSUM 22~1.0715G 4804 (2008) (JP)
Latvia11SMn301.0715EN 10087 (09/1998) (LV)
Latvia11SMn301.0715EN 10277-3 (03/2008) (LV)
Lithuania11SMn301.0715EN 10087 (09/1998) (LT)
Lithuania11SMn301.0715EN 10277-3 (03/2008) (LT)
Luxemburg11SMn301.0715EN 10087 (09/1998) (LU)
Luxemburg11SMn301.0715EN 10277-3 (03/2008) (LU)
Malta11SMn301.0715EN 10087 (09/1998) (MT)
Malta11SMn301.0715EN 10277-3 (03/2008) (MT)
Netherlands11SMn301.0715EN 10087 (09/1998) (NL)
Netherlands11SMn301.0715EN 10277-3 (03/2008) (NL)
Norway11SMn301.0715EN 10087 (09/1998) (NO)
Norway11SMn301.0715EN 10277-3 (03/2008) (NO)
Poland11SMn301.0715EN 10087 (09/1998) (PL)
Poland11SMn301.0715EN 10277-3 (03/2008) (PL)
PolandA10X1.071584026 (1973) withdrawn (PL)
Portugal11SMn301.0715EN 10087 (09/1998) (PT)
Portugal11SMn301.0715EN 10277-3 (03/2008) (PT)
Republic of KoreaSUM 22~1.0715D 3567 (2002) (KR)
Romania11SMn301.0715EN 10087 (09/1998) (RO)
Romania11SMn301.0715EN 10277-3 (03/2008) (RO)
Serbia11SMn301.0715EN 10087 (09/1998) (CS)
Serbia11SMn301.0715EN 10277-3 (03/2008) (CS)
SerbiaC39901.0715C.B0.505 (1984) withdrawn (CS)
Slovakia 11109~1.0715411109 (1974) (SK)
Slovakia11SMn301.0715EN 10087 (09/1998) (SK)
Slovakia11SMn301.0715EN 10277-3 (03/2008) (SK)
Slovenia11SMn301.0715EN 10087 (09/1998) (SL)
Slovenia11SMn301.0715EN 10277-3 (03/2008) (SL)
Spain11SMn301.0715EN 10087 (09/1998) (ES)
Spain11SMn301.0715EN 10277-3 (03/2008) (ES)
SpainF.210.A~1.0715Non standardized steels (ES)
SpainF.210.L~1.0715Non standardized steels (ES)
Spain11SMn 281.071536021 (1980) withdrawn (ES)
SpainF.21111.071536021 (1980) withdrawn (ES)
Sweden11SMn301.0715EN 10087 (09/1998) (SE)
Sweden11SMn301.0715EN 10277-3 (03/2008) (SE)
Sweden1912~1.0715141912withdrawn (SE)
Switzerland11SMn301.0715EN 10087 (09/1998) (CH)
Switzerland11SMn301.0715EN 10277-3 (03/2008) (CH)
Turkey11SMn301.0715EN 10087 (09/1998) (TR)
Turkey11SMn301.0715EN 10277-3 (03/2008) (TR)
U.S.A.G12130 (UNS)~1.0715
U.S.A.G12150 (UNS)~1.0715
U.S.A.1213 (AISI)~1.0715
U.S.A.1215 (AISI)~1.0715
U.S.A.A 29 (1213) (ASTM)~1.0715A29-05(US)
U.S.A.A 29 (1215) (ASTM)~1.0715A29-05(US)
U.S.A.A 108 (1213) (ASTM)~1.0715A 108-07(US)
U.S.A.A 108 (1215) (ASTM)~1.0715A 108-07(US)
U.S.A.A 510 (1213) (ASTM)~1.0715A510-07/06(US)
U.S.A.A 510 (1215) (ASTM)~1.0715A510-07/06(US)
U.S.A.A 519 (1213) (ASTM)~1.0715A519-06(US)
U.S.A.A 519 (1215) (ASTM)~1.0715A519-06(US)
U.S.A.A 521 (1215) (ASTM)~1.0715A 521-06(US)
U.S.A.A 521 (1213) (ASTM)~1.0715A 521-06(US)
U.S.A.A 576 (1213) (ASTM)~1.0715A 576-90 (06)(US)
U.S.A.A 576 (1215) (ASTM)~1.0715A 576-90 (06)(US)
U.S.A.A 711 (1213) (ASTM)~1.0715A 711-07(US)
U.S.A.A 711 (1215) (ASTM)~1.0715A 711-07(US)
U.S.A.1213 (SAE)~1.0715J 403 (2001) (US)
U.S.A.1215 (SAE)~1.0715J 403 (2001) (US)

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey