AISI 3140 Low Alloy Steel

AISI 3140 Low Alloy Steel

AISI 3140 Steel Overview

AISI 3140 steel (UNS G31400, EN 40NiCr6) is a low alloy steel. This page lists the AISI 3140 material data sheets for 2 conditions: annealed, normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 3140 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 3140 Steel Chemical Composition

C (carbon)0.38 – 0.43 %
Cr (chromium)0.55 – 0.75 %
Fe (iron)96.1 – 97.1 %
Mn (manganese)0.7 – 0.9 %
Ni (nickel)1.1 – 1.4 %
P (phosphorus)0 – 0.04 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.35 %

AISI 3140 Steel Material Data Sheets

AISI 3140 Annealed Material Data Sheet

AISI 3140 Normalized Material Data Sheet

AISI 3140 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 3140 Annealed vs Normalized: Yield, Tensile & Hardness Compared.

AISI 3140 Steel Parts from Turkey

Looking for AISI 3140 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 3140 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.