1.0736 Material Data Sheet: Non alloy quality steels

1.0736 Material Data Sheet: Non alloy quality steels: Steels with higher P or S content

Material Number1.0736
Steel groupNon alloy quality steels: Steels with higher P or S content
Symbol11SMn37; 9 SMn 36
StandardsDIN EN 10087 (01/1999) Free-cutting steels – Technical delivery conditions for semi-finished products, hot-rolled bars and rods.

DIN EN 10277-3 (06/2008) Bright steel products. Free-cutting steels. Steels not intended for heat treatment

Range of application: Free-cutting steels: Heavy duty free-cutting steel

1.0736 Material Composition

ElementMin/Max
C <=0.14
Si<=0.05
Mn1.00 – 1.50
P<=0.110
S0.340 – 0.400
Key Additives: Mn + S

1.0736 Standard Comparison

CountrySymbolMaterial No.Standard
Australia1214~1.07361442 (2007) (AU)
AustraliaS1214~1.07361448 (2007) (AU)
Austria11SMn371.0736EN 10087 (09/1998) (AT)
Austria11SMn371.0736EN 10277-3 (03/2008) (AT)
Belgium11SMn371.0736EN 10087 (09/1998) (BE)
Belgium11SMn371.0736EN 10277-3 (03/2008) (BE)
Bulgaria11SMn371.0736EN 10087 (09/1998) (BG)
Bulgaria11SMn371.0736EN 10277-3 (03/2008) (BG)
Cyprus11SMn371.0736EN 10087 (09/1998) (CY)
Cyprus11SMn371.0736EN 10277-3 (03/2008) (CY)
Czech Republic11SMn371.0736EN 10087 (09/1998) (CZ)
Czech Republic11SMn371.0736EN 10277-3 (03/2008) (CZ)
Denmark11SMn371.0736EN 10087 (09/1998) (DK)
Denmark11SMn371.0736EN 10277-3 (03/2008) (DK)
Estonia11SMn371.0736EN 10087 (09/1998) (EE)
Estonia11SMn371.0736EN 10277-3 (03/2008) (EE)
Europe11SMn371.073610087 (09/1998) (EUR)
Europe11SMn371.073610277-3 (03/2008) (EUR)
Finland11SMn371.0736EN 10087 (09/1998) (Fl)
Finland11SMn371.0736EN 10277-3 (03/2008) (Fl)
France11SMn371.0736EN 10087 (09/1998) (FR)
France11SMn371.0736EN 10277-3 (03/2008) (FR)
FranceS 3001.0736A35-561 (1992) withdrawn (FR)
FranceS 3001.0736A35-562 (1986) withdrawn (FR)
Great Britain11SMn371.0736EN 10087 (09/1998) (GB)
Great Britain11SMn371.0736EN 10277-3 (03/2008) (GB)
Greece11SMn371.0736EN 10087 (09/1998) (GR)
Greece11SMn371.0736EN 10277-3 (03/2008) (GR)
Hungary11SMn371.0736EN 10087 (09/1998) (HU)
Hungary11SMn371.0736EN 10277-3 (03/2008) (HU)
Iceland11SMn371.0736EN 10087 (09/1998) (IS)
Iceland11SMn371.0736EN 10277-3 (03/2008) (IS)
Ireland11SMn371.0736EN 10087 (09/1998) (IE)
Ireland11SMn371.0736EN 10277-3 (03/2008) (IE)
ISO12SMn35~(1.0736)683-9 (1988) (ISO)
Italy11SMn371.0736EN 10087 (09/1998) (IT)
Italy11SMn371.0736EN 10277-3 (03/2008) (IT)
JapanSUM 25~1.0736G 4804 (2008) (JP)
Latvia11SMn371.0736EN 10087 (09/1998) (LV)
Latvia11SMn371.0736EN 10277-3 (03/2008) (LV)
Lithuania11SMn371.0736EN 10087 (09/1998) (LT)
Lithuania11SMn371.0736EN 10277-3 (03/2008) (LT)
Luxemburg11SMn371.0736EN 10087 (09/1998) (LU)
Luxemburg11SMn371.0736EN 10277-3 (03/2008) (LU)
Malta11SMn371.0736EN 10087 (09/1998) (MT)
Malta11SMn371.0736EN 10277-3 (03/2008) (MT)
Netherlands11SMn371.0736EN 10087 (09/1998) (NL)
Netherlands11SMn371.0736EN 10277-3 (03/2008) (NL)
Norway11SMn371.0736EN 10087 (09/1998) (NO)
Norway11SMn371.0736EN 10277-3 (03/2008) (NO)
Poland11SMn371.0736EN 10087 (09/1998) (PL)
Poland11SMn371.0736EN 10277-3 (03/2008) (PL)
Portugal11SMn371.0736EN 10087 (09/1998) (PT)
Portugal11SMn371.0736EN 10277-3 (03/2008) (PT)
Republic of KoreaSUM 25~1.0736D 3567 (2002) (KR)
Romania11SMn371.0736EN 10087 (09/1998) (RO)
Romania11SMn371.0736EN 10277-3 (03/2008) (RO)
Serbia11SMn371.0736EN 10087 (09/1998) (CS)
Serbia11SMn371.0736EN 10277-3 (03/2008) (CS)
SerbiaC39911.0736C.B0.505 (1984) withdrawn (CS)
Slovak Republic11SMn371.0736EN 10087 (09/1998) (SK)
Slovak Republic11SMn371.0736EN 10277-3 (03/2008) (SK)
Slovenia11SMn371.0736EN 10087 (09/1998) (SL)
Slovenia11SMn371.0736EN 10277-3 (03/2008) (SL)
Spain11SMn371.0736EN 10087 (09/1998) (ES)
Spain11SMn371.0736EN 10277-3 (03/2008) (ES)
Spain12 SMn 351.073636021 (1980) withdrawn (ES)
SpainF.21131.073636021 (1980) withdrawn (ES)
Sweden11SMn371.0736EN 10087 (09/1998) (SE)
Sweden11SMn371.0736EN 10277-3 (03/2008) (SE)
Switzerland11SMn371.0736EN 10087 (09/1998) (CH)
Switzerland11SMn371.0736EN 10277-3 (03/2008) (CH)
Turkey11SMn371.0736EN 10087 (09/1998) (TR)
Turkey11SMn371.0736EN 10277-3 (03/2008) (TR)
U.S.A.G12150 (UNS)~1.0736
U.S.A.1215 (AISI)~1.0736
U.S.A.A 29 (1215) (ASTM)~1.0736A 29-05(US)
U.S.A.A 108 (1215) (ASTM)~1.0736A 108-07(US)
U.S.A.A 510 (1215) (ASTM)~1.0736A 510-07/06(US)
U.S.A.A 519 (1215) (ASTM)~1.0736A 519-06(US)
U.S.A.A 521 (1215) (ASTM)~1.0736A 521-06(US)
U.S.A.A 576 (1215) (ASTM)~1.0736A 576-90 (06)(US)
U.S.A.A 711(1215) (ASTM)~1.0736A 711-07(US)
U.S.A.1215 (SAE) ~1.0736J 403 (2001) (US)

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey