| AISI 1144, Carbon steel Resulfurized, 0.44% C | Equivalent Grades |
|---|---|
| UNS number | G11440 |
| US name | ASTM G11440, ASTM 1144 Class B, ASTM 1144 Class A, ASTM 1144 |
| UK name | 226M44 to BS 970/3, 44SMn28 to BS EN 10277-3, 44SMnPb28 to BS EN 10277-3 |
| Italy name | CF44SMn28 to UNI 4838, CF44SMnPb28 to UNI 4838 |
| JIS (Japanese) name | SUM43 |
Tradenames of AISI 1144, Carbon steel ( Resulfurized, 0.44% C ): C1144 MOD, ELASTUF STRAINFREE, JALCASE 10, JALCASE 100, JALCASE 9, LASALLE 1144, RYTENSE 44, S-1144, SAARSTAHL SAE 1144, STRAIN TEMPERED 1144, STRESS-PROOF NO. 1, STRESS-PROOF NO. 2, STRESS-PROOF NO. 3, WYCO 100-44, WYCO 125-44
| Standards with similar compositions: |
|---|
| BDS 6886 A45 (Bulgaria) |
| GB 8731(88) Y40Mn (China) |
| AFNOR NFA35562 45MF6 (France) |
| JIS G4804(83) SUM43 (Japan) |
| NMX-B-301(86) 1144 (Mexico) |
| AS 1442 XK1145 (NSW Australia) |
| AS 1442 XK1152 (NSW Australia) |
| AS 1442(92) 1144 (NSW Australia) |
| AS 1443 XK1152 (NSW Australia) |
| AS 1443(94) 1144 (NSW Australia) |
| PNH84026 A45 (Poland) |
| STAS 1350(89) AUT40Mn (Romania) |
| UNE 36021(61) 45MnS6 (Spain) |
| UNE 36021(61) F.2133 (Spain) |
| BS 970/1(83) 212A42 (United Kingdom) |
| BS 970/1(83) 216M44 (United Kingdom) |
| BS 970/3(91) 226M44 (United Kingdom) |
| ASTM A108(95) 1144 (USA) |
| ASTM A29/A29M(93) 1144 (USA) |
| ASTM A311/A311M(95) 1144 Class A (USA) |
| ASTM A311/A311M(95) 1144 Class B (USA) |
| ASTM A510(96) 1144 (USA) |
| ASTM A519(96) 1144 (USA) |
| ASTM A576(95) 1144 (USA) |
| FED QQ-S-637A(70) C1144 (USA) |
| SAE J1397(92) 1144 (USA) |
| SAE J403(95) 1144 (USA) |
| 1144 (USA) |
| AISI 1144 (USA) |
| COPANT 330 1444 (Venezuela) |
| COPANT 331 1444 (Venezuela) |
| COPANT 332 1444 (Venezuela) |
| C.1590 (Yugoslavia) |
• Australia:
1144 to AS 1442, 1144 to AS 1443
• Italy:
CF44SMn28 to UNI 4838, CF44SMnPb28 to UNI 4838
• Japan:
SUM43 to JIS G4804
• Mexico:
1144 to NMX-B-301
• Pan America:
1444 to COPANT 330, 1444 to COPANT 331, 1444 to COPANT 332
• Russia:
AS45G2 to GOST 1414
• UK:
226M44 to BS 970/3, 44SMn28 to BS EN 10277-3, 44SMnPb28 to BS EN 10277-3
• USA:
1144, 1144 Class A to ASTM A311/A311M, 1144 Class B to ASTM A311/A311M, 1144 to ASTM A29/A29M, 1144 to ASTM A519, 1144 to SAE J403, 11L44, C1144 to FED QQ-S-637A, G11440 to ASTM A510/A510M, G11440 to ASTM A576-90b, UNS G11440