| EN 582:1993 | Thermal spraying – Determination of tensile adhesive strength |
| EN 657:2005 | Thermal spraying – Terminology, classification |
| EN 1274:2004 | Thermal spraying – Powders – Composition, technical supply conditions |
| EN 1395-1:2007 | Thermal spraying – Acceptance inspection of thermal spraying equipment – Part 1: General requirements |
| EN 1395-2:2007 | Thermal spraying – Acceptance inspection of thermal spraying equipment – Part 2: Flame spraying including HVOF |
| EN 1395-3:2007 | Thermal spraying – Acceptance inspection of thermal spraying equipment – Part 3: Arc spraying |
| EN 1395-4:2007 | Thermal spraying – Acceptance inspection of thermal spraying equipment – Part 4: Plasma spraying |
| EN 1395-5:2007 | Thermal spraying – Acceptance inspection of thermal spraying equipment – Part 5: Plasma spraying in chambers |
| EN 1395-6:2007 | Thermal spraying – Acceptance inspection of thermal spraying equipment – Part 6: Manipulator systems |
| EN 1395-7:2007 | Thermal spraying – Acceptance inspection of thermal spraying equipment – Part 7: Powder feed systems |
| EN ISO 2063:2005 | Thermal spraying – Metallic and other inorganic coatings – Zinc, aluminium and their alloys (ISO 2063:2005) |
| EN ISO 12670:2015 | Thermal spraying – Components with thermally sprayed coatings – Technical supply conditions (ISO 12670:2011) |
| EN ISO 12671:2014 | Thermal spraying – Thermally sprayed coatings – Symbolic representation on drawings (ISO 12671:2012) |
| EN ISO 12679:2015 | Thermal spraying – Recommendations for thermal spraying (ISO 12679:2011) |
| EN ISO 12690:2010 | Metallic and other inorganic coatings – Thermal spray coordination – Tasks and responsibilities (ISO 12690:2010) |
| EN ISO 13123:2011 | Metallic and other inorganic coatings – Test method of cyclic heating for thermal-barrier coatings under temperature gradient (ISO 13123:2011) |
| EN 13507:2010 | Thermal spraying – Pre-treatment of surfaces of metallic parts and components for thermal spraying |
| EN 14616:2004 | Thermal spraying – Recommendations for thermal spraying |
| EN ISO 14918:1998 | Thermal spraying – Approval testing of thermal sprayers (ISO 14918:1998) |
| EN ISO 14919:2015 | Thermal spraying – Wires, rods and cords for flame and arc spraying – Classification – Technical supply conditions (ISO 14919:2015) |
| EN ISO 14920:2015 | Thermal spraying – Spraying and fusing of self-fluxing alloys (ISO 14920:2015) |
| EN ISO 14921:2010 | Thermal spraying – Procedures for the application of thermally sprayed coatings for engineering components (ISO 14921:2010) |
| EN ISO 14922-1:1999 | Thermal spraying – Quality requirements of thermally sprayed structures – Part 1: Guidance for selection and use (ISO 14922-1:1999) |
| EN ISO 14922-2:1999 | Thermal spraying – Quality requirements of thermally sprayed structures – Part 2: Comprehensive quality requirements (ISO 14922-2:1999) |
| EN ISO 14922-3:1999 | Thermal spraying – Quality requirements of thermally sprayed structures – Part 3: Standard quality requirements (ISO 14922-3:1999) |
| EN ISO 14922-4:1999 | Thermal spraying – Quality requirements of thermally sprayed structures – Part 4: Elementary quality requirements (ISO 14922-4:1999) |
| EN ISO 14923:2003 | Thermal spraying – Characterization and testing of thermally sprayed coatings (ISO 14923:2003) |
| EN ISO 14924:2005 | Thermal spraying – Post-treatment and finishing of thermally sprayed coatings (ISO 14924:2005) |
| EN 15311:2007 | Thermal spraying – Components with thermally sprayed coatings – Technical supply conditions |
| CEN/TR 15339-1:2014 | Thermal spraying – Safety requirements for thermal spraying equipment – Part 1: General requirements |
| EN 15339-2:2007 | Thermal spraying – Safety requirements for thermal spraying equipment – Part 2: Gas control units |
| CEN/TR 15339-3:2014 | Thermal spraying – Safety requirements for thermal spraying equipment – Part 3: Torches for thermal spraying and their connection and supply units |
| CEN/TR 15339-4:2014 | Thermal spraying – Safety requirements for thermal spraying equipment – Part 4: Gas and liquid fuel supply |
| CEN/TR 15339-5:2014 | Thermal spraying – Safety requirements for thermal spraying equipment – Part 5: Powder and wire feed units |
| CEN/TR 15339-6:2014 | Thermal spraying – Safety requirements for thermal spraying equipment – Part 6: Spray booth, Handling system, Dust collection, Exhaust system, Filter |
| EN 15340:2007 | Thermal spraying – Determination of shear load resistance of thermally sprayed coatings |
| EN 15520:2007 | Thermal spraying – Recommendations for constructional design of components with thermally sprayed coatings |
| EN 15648:2009 | Thermal spraying – Component related procedure qualification |
| EN 16813:2016 | Thermal spraying – Measurement of the electrical conductivity of thermal sprayed non-iron metal coatings by means of eddy current method |
| EN ISO 17834:2003 | Thermal spraying – Coatings for protection against corrosion and oxidation at elevated temperatures (ISO 17834:2003) |
| EN ISO 17836:2004 | Thermal spraying – Determination of the deposition efficiency for thermal spraying (ISO 17836:2004) |