AISI 4135 Low Alloy Steel

AISI 4135 Low Alloy Steel

AISI 4135 Steel Overview

AISI 4135 steel (UNS G41350, EN 34CrMo4) is a low alloy steel. This page lists the AISI 4135 material data sheets for 2 conditions: normalized, air melted, quenched & tempered. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 4135 Steel

General construction, general mechanical engineering, automotive, pressure vessels, pipework

AISI 4135 Steel Chemical Composition

C (carbon)0.33 – 0.38 %
Cr (chromium)0.8 – 1.1 %
Fe (iron)96.9 – 97.9 %
Mn (manganese)0.7 – 0.9 %
Mo (molybdenum)0.15 – 0.25 %
P (phosphorus)0 – 0.035 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.35 %

AISI 4135 Steel Material Data Sheets

AISI 4135 Normalized Material Data Sheet

AISI 4135 Air Melted, Quenched & Tempered Material Data Sheet

AISI 4135 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 4135 Normalized vs Quenched & Tempered: Yield, Tensile & Hardness Compared.