AISI 1118 Resulfurized Low Carbon Steel

AISI 1118 Resulfurized Low Carbon Steel

AISI 1118 Steel Overview

AISI 1118 steel (UNS G11180) is a resulfurized low carbon steel. AISI 1118 is a free-machining grade: its raised sulfur content gives short chips and fast cutting speeds. This page lists the AISI 1118 material data sheets for 3 conditions: annealed, as rolled, normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 1118 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 1118 Steel Chemical Composition

C (carbon)0.14 – 0.2 %
Fe (iron)98 – 98.5 %
Mn (manganese)1.3 – 1.6 %
P (phosphorus)0 – 0.04 %
S (sulfur)0.08 – 0.13 %

AISI 1118 Steel Material Data Sheets

AISI 1118 Annealed Material Data Sheet

AISI 1118 As Rolled Material Data Sheet

AISI 1118 Normalized Material Data Sheet

AISI 1118 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 1118 Annealed vs As Rolled vs Normalized: Yield, Tensile & Hardness Compared.

AISI 1118 Compared with Other Resulfurized Steels

Compare the composition, mechanical properties and machining speed of AISI 1118 with AISI 1117, 1118, 12L14, 1137, 1141 and 1144 in our resulfurized free-machining steels comparison.

AISI 1118 Steel Parts from Turkey

Looking for AISI 1118 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1118 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low carbon steel grades.