Aluminum A360.0 Mechanical Properties (Die cast, F)

Aluminum A360.0 Mechanical Properties

Young’s modulus69.6–72.4GPa
Specific stiffness25.9–27MN.m/kg
Yield strength (elastic limit)157–173MPa
Tensile strength317–349MPa
Specific strength58.3–64.6kN.m/kg
Elongation5–6% strain
Compressive strength157–173MPa
Flexural modulus69.6–72.4GPa
Flexural strength (modulus of rupture)165–182MPa
Shear modulus26–27.4GPa
Bulk modulus65.2–74.5GPa
Poisson’s ratio0.322–0.338 
Shape factor34   
Hardness – Vickers87–97HV
Elastic stored energy (springs)173–211kJ/m^3
Fatigue strength at 10^7 cycles112–136MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles108–141MPa

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treatment, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey