AISI 8660 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 8660 Oil Quenched & Tempered at 650°C Material Data Sheet

AISI 8660 Oil Quenched & Tempered at 650°C Overview

AISI 8660 tempered 650°C is AISI 8660 low alloy steel (UNS G86600) in the oil quenched & tempered at 650°C condition. This AISI 8660 tempered 650°C material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 8660 conditions in our AISI 8660 yield, tensile and hardness comparison. Looking for AISI 8660 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 8660 steel parts in-house and inspects them before shipment.

AISI 8660 Oil Quenched & Tempered at 650°C Designation

AISI 8660
ConditionTempered at 650°C & oil quenched
UNS numberG86600
US nameSAE 8660H, SAE 8660, ASTM G86600, ASTM 8660H, ASTM 8660

AISI 8660 Oil Quenched & Tempered at 650°C Typical uses

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 8660 Oil Quenched & Tempered at 650°C Composition detail

C (carbon)0.55–0.65%
Cr (chromium)0.4–0.6%
Fe (iron)96.4–97.6%
Mn (manganese)0.75–1%
Mo (molybdenum)0.15–0.25%
Ni (nickel)0.4–0.7%
P (phosphorus)0–0.035%
S (sulfur)0–0.04%
Si (silicon)0.15–0.35%

AISI 8660 Oil Quenched & Tempered at 650°C Physical properties

Density7.8–7.9g/cm3

AISI 8660 Oil Quenched & Tempered at 650°C Mechanical properties

Young’s modulus201–212GPa
Specific stiffness25.6–27MN.m/kg
Yield strength (elastic limit)855–1050MPa
Tensile strength955–1180MPa
Specific strength109–133kN.m/kg
Elongation16–24% strain
Compressive strength855–1050MPa
Flexural modulus201–212GPa
Flexural strength (modulus of rupture)855–1050MPa
Shear modulus77–83GPa
Bulk modulus155–173GPa
Poisson’s ratio0.285–0.295 
Shape factor26
Hardness – Vickers280–350HV
Elastic stored energy (springs)1780–2620kJ/m3
Fatigue strength at 10^7 cycles414–481MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
360–554MPa

AISI 8660 Oil Quenched & Tempered at 650°C Impact & fracture properties

Fracture toughness41–70MPa.m0.5
Toughness (G)8.61–22.4kJ/m2

AISI 8660 Oil Quenched & Tempered at 650°C Thermal properties

Melting point1380–1490°C
Maximum service temperature587–640°C
Minimum service temperature-63–-38°C
Thermal conductivity34–44W/m.°C
Specific heat capacity460–500J/kg.°C
Thermal expansion coefficient11–13µstrain/°C
Thermal shock resistance336–436°C
Thermal distortion resistance2.78–3.76MW/m
Latent heat of fusion265–280kJ/kg

AISI 8660 Oil Quenched & Tempered at 650°C Electrical properties

Electrical resistivity23–35µohm.cm
Electrical conductivity4.93–7.5%IACS
Galvanic potential-0.5–-0.42V

AISI 8660 Oil Quenched & Tempered at 650°C Magnetic properties

Magnetic typeMagnetic

AISI 8660 Oil Quenched & Tempered at 650°C Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5060–5200m/s
Mechanical loss coefficient (tan delta)3.7e-4–4.7e-4 

AISI 8660 Oil Quenched & Tempered at 650°C Processing properties

Metal castingUnsuitable
Metal cold formingExcellent
Metal hot formingExcellent
Metal press formingExcellent
Metal deep drawingLimited use
Machining speed14.9 m/min
Weldability
Notes: Preheating and post weld heat treatments are required
Poor
Carbon equivalency0.812 – 1.03

AISI 8660 Oil Quenched & Tempered at 650°C Durability

Water (fresh)Acceptable
Water (salt)Limited use
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CAcceptable
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)Acceptable
FlammabilityNon-flammable

AISI 8660 Oil Quenched & Tempered at 650°C Corrosion resistance

Stress corrosion cracking
Note: Rated in chloride; May be susceptible in halide, ammonia, nitrogen, acidic, caustic, carbonate environments
Slightly susceptible

AISI 8660 Oil Quenched & Tempered at 650°C Standards with similar compositions

Australia: 8660 to AS 1444, 8660H to AS 1444
Mexico: 8660 to NMX-B-203-SCFI, 8660 to NMX-B-300, 8660H to NMX-B-268, 8660H to NMX-B-300
Pan America: 8660 to COPANT 334, 8660 to COPANT 514
UK: 805A60 to BS 970/1, 805H60 to BS 970/1, 805H60 to BS 970/2
USA: 8660, 8660 to ASTM A29/A29M, 8660 to ASTM A519, 8660 to SAE J770, 8660H, 8660H to ASTM A304, 8660H to ASTM A331-95, 8660H to SAE J1268, G86600 to ASTM A1031, UNS G86600, UNS H86600
Tradenames: VB-60