AM-355 SCT 850 Stainless Steel Material Data Sheet

AM-355 SCT 850 Stainless Steel Material Data Sheet (Semi-austenitic, Precipitation Hardened)

AM-355 SCT 850 Stainless Steel Overview

AM-355 SCT 850 stainless steel is a semi-austenitic precipitation hardening stainless steel (UNS S35500) in the wrought form. Condition: SCT 850 (Solution annealed; hardened by sub-zero cooling and tempering at 455°C). This AM-355 SCT 850 stainless steel material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for AM-355 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AM-355 parts in-house and inspects them before shipment.

AM-355 Designation

AM-355, wrought
ConditionSCT 850 (Solution annealed; hardened by sub-zero cooling and tempering at 455°C)
UNS numberS35500
US nameAM-355

AM-355 Typical uses

Processing of potentially corrosive liquids e.g. chemicals/oil/beverages/sewage, structural uses in corrosive environments, e.g. nuclear plants, ships, offshore oil installations, underwater cables and pipes

AM-355 SCT 850 Stainless Steel Composition detail

C (carbon)0.1–0.15%
Cr (chromium)15–16%
Fe (iron)73.6–77.8%
Mn (manganese)0.5–1.25%
Mo (molybdenum)2.5–3.25%
N (nitrogen)0.07–0.13%
Ni (nickel)4–5%
P (phosphorus)0–0.04%
S (sulfur)0–0.03%
Si (silicon)0–0.5%

AM-355 Physical properties

Density7.77–7.84g/cm3

AM-355 SCT 850 Stainless Steel Mechanical properties

Young’s modulus200–210GPa
Specific stiffness25.6–26.9MN.m/kg
Yield strength (elastic limit)1120–1230MPa
Tensile strength1300–1430MPa
Specific strength143–158kN.m/kg
Elongation2–8% strain
Compressive strength1240–1370MPa
Flexural modulus200–210GPa
Flexural strength (modulus of rupture)1120–1230MPa
Shear modulus76–79.9GPa
Bulk modulus185–195GPa
Poisson’s ratio0.32–0.333 
Shape factor20
Hardness – Vickers350–380HV
Hardness – Rockwell B115–117HRB
Hardness – Rockwell C45–50HRC
Hardness – Brinell426–472HB
Elastic stored energy (springs)3040–3720kJ/m3
Fatigue strength at 10^7 cycles518–620MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
495–649MPa

AM-355 Impact & fracture properties

Fracture toughness53.1–64.9MPa.m0.5
Toughness (G)13.9–20.4kJ/m2

AM-355 SCT 850 Stainless Steel Thermal properties

Melting point1400–1440°C
Maximum service temperature382–427°C
Minimum service temperature-73–-43°C
Thermal conductivity15.6–16.9W/m.°C
Specific heat capacity490–510J/kg.°C
Thermal expansion coefficient12.1–12.7µstrain/°C
Thermal shock resistance436–492°C
Thermal distortion resistance1.25–1.38MW/m
Latent heat of fusion308–379kJ/kg

AM-355 Electrical properties

Electrical resistivity75.3–104µohm.cm
Electrical conductivity1.65–2.29%IACS
Galvanic potential-0.21–-0.13V

AM-355 Magnetic properties

Magnetic typeMagnetic

AM-355 Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity5060–5190m/s
Mechanical loss coefficient (tan delta)3.1e-4–6.6e-4 

AM-355 Processing properties

Metal castingUnsuitable
Metal cold formingLimited use
Metal hot formingAcceptable
Metal press formingAcceptable
Metal deep drawingUnsuitable
Machining speed10.7 m/min
Weldability
Notes: Preheating is not required, post weld heat treatment is required
Good
Weldability – MIGGood
Weldability – plasmaGood
Weldability – SAWNot recommended
Weldability – TIGGood
BrazeabilityGood
Carbon equivalency3.95 – 4.54

AM-355 Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsAcceptable
Weak alkalisExcellent
Strong alkalisLimited use
Organic solventsExcellent
Oxidation at 500CExcellent
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)
Notes: Aluminum bronze is the most suitable mating material to minimize galling.
Limited use
FlammabilityNon-flammable

AM-355 SCT 850 Stainless Steel Corrosion resistance

Pitting resistance equivalent number (PREN)24.4 – 28.8
Pitting and crevice corrosionMedium (20-30)
Stress corrosion cracking
Note: Rated in chloride; Other susceptible environments: Hydrogen sulfide
Highly susceptible
Intergranular (weld line) corrosionGood
Inorganic acidsRestricted
Organic acidsModerate
AlkalisModerate
Humidity / waterExcellent
Sea waterRestricted
Sour oil and gasRestricted

AM-355 Notes

AM-355 SCT 850 Warning
Check with supplier what tempering and aging procedure has been applied – it could make a major difference to the steel’s mechanical properties.

AM-355 Standards with similar compositions

USA: 5549 to AMS 5549F, 64 to ASTM A579, AM-355 to SAE J467, S35500 to ASTM A564/A564M, S35500 to ASTM A705/A705M-95, UNS S35500, UNS S35580
Tradenames: AM 355, AM-355, CRONIFER 1505 MON – ALLOY 355, SLATER AM355, UNITEMP 355