| Mechanical properties | Values |
|---|---|
| Young’s modulus | * 193 – 201 GPa |
| Specific stiffness | * 24.7 – 25.7 MN.m/kg |
| Yield strength (elastic limit) | 324 – 415 MPa |
| Tensile strength | 662 – 795 MPa |
| Specific strength | * 41.5 – 53.1 kN.m/kg |
| Elongation | 52 – 62 % strain |
| Compressive strength | * 324 – 415 MPa |
| Flexural modulus | * 193 – 201 GPa |
| Flexural strength (modulus of rupture) | * 324 – 415 MPa |
| Shear modulus | 75 – 80 GPa |
| Poisson’s ratio | * 0.265 – 0.275 |
| Shape factor | 55 |
| Hardness – Vickers | * 192 – 230 HV |
| Hardness – Rockwell B | 90 – 96 HRB |
| Hardness – Rockwell C | * 9 – 18 HRC |
| Hardness – Brinell | * 185 – 214 HB |
| Elastic stored energy (springs) | * 309 – 511 kJ/m^3 |
| Fatigue strength at 10^7 cycles | 278 – 308 MPa |
| Fatigue strength model (stress range) | * 243 – 352 MPa |
| *Values indicated with asterisks (*) are approximate. No guarantee is provided for the precision of this information. |