AISI 1030 Medium Carbon Steel

AISI 1030 Medium Carbon Steel

AISI 1030 Steel Overview

AISI 1030 steel (UNS G10300) is a medium carbon steel. This page lists the AISI 1030 material data sheets for 8 conditions: annealed, as rolled, normalized, water quenched & tempered at 205°C, water quenched & tempered at 315°C, water quenched & tempered at 425°C, water quenched & tempered at 540°C, water quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 1030 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 1030 Steel Chemical Composition

C (carbon)0.28 – 0.34 %
Fe (iron)98.7 – 99.1 %
Mn (manganese)0.6 – 0.9 %
P (phosphorus)0 – 0.04 %
S (sulfur)0 – 0.05 %

AISI 1030 Steel Material Data Sheets

AISI 1030 Annealed Material Data Sheet

AISI 1030 As Rolled Material Data Sheet

AISI 1030 Normalized Material Data Sheet

AISI 1030 Water Quenched & Tempered at 205°C Material Data Sheet

AISI 1030 Water Quenched & Tempered at 315°C Material Data Sheet

AISI 1030 Water Quenched & Tempered at 425°C Material Data Sheet

AISI 1030 Water Quenched & Tempered at 540°C Material Data Sheet

AISI 1030 Water Quenched & Tempered at 650°C Material Data Sheet

AISI 1030 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 1030 Annealed vs As Rolled vs Normalized vs Water Quenched & Tempered (205–650°C): Yield, Tensile & Hardness Compared.

AISI 1030 Steel Parts from Turkey

Looking for AISI 1030 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1030 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all medium and high carbon steel grades.