Low carbon steels, often called mild steels, contain roughly 0.05–0.25% carbon with manganese as the main other element. They are soft, ductile and easy to weld, cold form and machine, and they are the most widely used steels for sheet, bar, tube and general engineering parts. Low carbon steels cannot be usefully through-hardened by quenching; where a hard wear surface is needed, they are case hardened by carburizing or carbonitriding.
AISI and SAE Carbon Steel Numbering
In the AISI/SAE four-digit system, 10xx means plain carbon steel, 11xx means resulfurized carbon steel and 12xx means resulfurized and rephosphorized steel; an L, as in 12L14, shows a lead addition. The last two digits give the nominal carbon content in hundredths of a percent, so AISI 1020 contains about 0.20% carbon.
Low Carbon Steel Conditions: Annealed, As Rolled and Normalized
The data sheets below cover the annealed, as rolled and normalized conditions. Annealed low carbon steel is softest and most formable. As rolled material is supplied straight from hot rolling, and normalized steel has been reheated and air cooled for a finer, more uniform grain structure and slightly higher strength. A comparison post for each grade shows the yield strength, tensile strength and hardness side by side.
Free-Machining Low Carbon Steels
AISI 1117, 1118 and 12L14 are free-machining grades. Their raised sulfur, and the lead in 12L14, produce short chips and allow much higher cutting speeds on automatic lathes. Compare them with the medium carbon free-machining grades in our resulfurized free-machining steels comparison.
Low Carbon Steel Parts from Turkey
Looking for low carbon steel parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined low carbon steel parts in-house, including AISI 1020, 1117 and 12L14, and inspects them before shipment. For higher strength grades see medium and high carbon steel grades and low alloy steel grades.