1.0764 Material Data Sheet: Non alloy quality steels

1.0764 Material Data Sheet: Non alloy quality steels: Steels with higher P or S content

Material Number1.0764
Steel groupNon alloy quality steels: Steels with higher P or S content
Symbol36SMn14
StandardsDIN EN 10087 (01/1999) Free-cutting steels – Technical delivery conditions for semi-finished products, hot-rolled bars and rods.
Heat-treatable steels

DIN EN 10277-3 (06/2008) Bright steel products. Free-cutting steels. Steels for quenching and tempering

1.0764 Material Composition

ElementMin/Max
C0.32 – 0.39
Si<=0.40
Mn1.30 – 1.70
P<=0.060
S0.100 – 0.180

1.0764 Standard Comparison

Country                                                             Symbol          Material NoStandard
Austria36SMn141.0764EN 10087 (09/1998) (AT)
Austria36SMn141.0764EN 10277-3 (03/2008) (AT)
Belgium36SMn141.0764EN 10087 (09/1998) (BE)
Belgium36SMn141.0764EN 10277-3 (03/2008) (BE)
Bulgaria36SMn141.0764EN 10087 (09/1998) (BG)
Bulgaria36SMn141.0764EN 10277-3 (03/2008) (BG)
Cyprus36SMn141.0764EN 10087 (09/1998) (CY)
Cyprus36SMn141.0764EN 10277-3 (03/2008) (CY)
Czech Republic36SMn141.0764EN 10087 (09/1998) (CZ)
Czech Republic36SMn141.0764EN 10277-3 (03/2008) (CZ)
Denmark36SMn141.0764EN 10087 (09/1998) (DK)
Denmark36SMn141.0764EN 10277-3 (03/2008) (DK)
Estonia36SMn141.0764EN 10087 (09/1998) (EE)
Estonia36SMn141.0764EN 10277-3 (03/2008) (EE)
Europe36SMn141.076410087 (09/1998) (EUR)
Europe36SMn141.076410277-3 (03/2008) (EUR)
Finland36SMn141.0764EN 10087 (09/1998) (Fl)
Finland36SMn141.0764EN 10277-3 (03/2008) (Fl)
France36SMn141.0764EN 10087 (09/1998) (FR)
France36SMn141.0764EN 10277-3 (03/2008) (FR)
Great Britain36SMn141.0764EN 10087 (09/1998) (GB)
Great Britain36SMn141.0764EN 10277-3 (03/2008) (GB)
Great Britain216 M 36 t1.0764970 Part 1 (1996) withdrawn (GB)
Greece36SMn141.0764EN 10087 (09/1998) (GR)
Greece36SMn141.0764EN 10277-3 (03/2008) (GR)
Hungary36SMn141.0764EN 10087 (09/1998) (HU)
Hungary36SMn141.0764EN 10277-3 (03/2008) (HU)
Iceland36SMn141.0764EN 10087 (09/1998) (IS)
Iceland36SMn141.0764EN 10277-3 (03/2008) (IS)
India40Mn15S12-1.07643930 (1994) (IN)
Ireland36SMn141.0764EN 10087 (09/1998) (IE)
Ireland36SMn141.0764EN 10277-3 (03/2008) (IE)
Italy36SMn141.0764EN 10087 (09/1998) (IT)
Italy36SMn141.0764EN 10277-3 (03/2008) (IT)
Latvia36SMn141.0764EN 10087 (09/1998) (LV)
Latvia36SMn141.0764EN 10277-3 (03/2008) (LV)
Lithuania36SMn141.0764EN 10087 (09/1998) (LT)
Lithuania36SMn141.0764EN 10277-3 (03/2008) (LT)
Luxemburg36SMn141.0764EN 10087 (09/1998) (LU)
Luxemburg36SMn141.0764EN 10277-3 (03/2008) (LU)
Malta36SMn141.0764EN 10087 (09/1998) (MT)
Malta36SMn141.0764EN 10277-3 (03/2008) (MT)
Netherlands36SMn141.0764EN 10087 (09/1998) (NL)
Netherlands36SMn141.0764EN 10277-3 (03/2008) (NL)
Norway36SMn141.0764EN 10087 (09/1998) (NO)
Norway36SMn141.0764EN 10277-3 (03/2008) (NO)
Poland36SMn141.0764EN 10087 (09/1998) (PL)
Poland36SMn141.0764EN 10277-3 (03/2008) (PL)
Portugal36SMn141.0764EN 10087 (09/1998) (PT)
Portugal36SMn141.0764EN 10277-3 (03/2008) (PT)
Romania36SMn141.0764EN 10087 (09/1998) (RO)
Romania36SMn141.0764EN 10277-3 (03/2008) (RO)
Serbia36SMn141.0764EN 10087 (09/1998) (CS)
Serbia36SMn141.0764EN 10277-3 (03/2008) (CS)
Slovakia36SMn141.0764EN 10087 (09/1998) (SK)
Slovakia36SMn141.0764EN 10277-3 (03/2008) (SK)
Slovenia36SMn141.0764EN 10087 (09/1998) (SL)
Slovenia36SMn141.0764EN 10277-3 (03/2008) (SL)
Spain36SMn141.0764EN 10087 (09/1998) (ES)
Spain36SMn141.0764EN 10277-3 (03/2008) (ES)
Sweden36SMn141.0764EN 10087 (09/1998) (SE)
Sweden36SMn141.0764EN 10277-3 (03/2008) (SE)
Switzerland36SMn141.0764EN 10087 (09/1998) (CH)
Switzerland36SMn141.0764EN 10277-3 (03/2008) (CH)
Turkey36SMn141.0764EN 10087 (09/1998) (TR)
Turkey36SMn141.0764EN 10277-3 (03/2008) (TR)

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey