1.0762 Material Data Sheet: Non alloy quality steels

1.0762 Material Data Sheet: Non alloy quality steels: Steels with higher P or S content

Material Number1.0762
Steel groupNon alloy quality steels: Steels with higher P or S content
Symbol44SMn28
StandardsDIN EN 10087 (01/1999) Free-cutting steels – Technical delivery conditions for semi-finished products, hot-rolled bars and rods.
Heat-treatable steels

DIN EN 10277-3 (06/2008) Bright steel products. Free-cutting steels. Steels for quenching and tempering

Range of application: Free-cutting steels: Free-cutting heat-treatable steel

1.0762 Material Composition

ElementMin/Max
C0.40 – 0.48
Si<=0.40
Mn1.30 – 1.70
P<=0.060
S0.240 – 0.330
High Carbon Content: Gives strength and hardness after heat treatmentKey Additives: Mn + S

1.0762 Standard Comparison

Australia1144~1.07621443 (2004) (AU)
Austria44SMn281.0762EN 10087 (09/1998) (AT)
Austria44SMn281.0762EN 10277-3 (03/2008) (AT)
Belgium44SMn281.0762EN 10087 (09/1998) (BE)
Belgium44SMn281.0762EN 10277-3 (03/2008) (BE)
Bulgaria44SMn281.0762EN 10087 (09/1998) (BG)
Bulgaria44SMn281.0762EN 10277-3 (03/2008) (BG)
Cyprus44SMn281.0762EN 10087 (09/1998) (CY)
Cyprus44SMn281.0762EN 10277-3 (03/2008) (CY)
Czech Republic44SMn281.0762EN 10087 (09/1998) (CZ)
Czech Republic44SMn281.0762EN 10277-3 (03/2008) (CZ)
Denmark44SMn281.0762EN 10087 (09/1998) (DK)
Denmark44SMn281.0762EN 10277-3 (03/2008) (DK)
Estonia44SMn281.0762EN 10087 (09/1998) (EE)
Estonia44SMn281.0762EN 10277-3 (03/2008) (EE)
Europe44SMn281.076210087 (09/1998) (EUR)
Europe44SMn281.076210277-3 (03/2008) (EUR)
Finland44SMn281.0762EN 10087 (09/1998) (Fl)
Finland44SMn281.0762EN 10277-3 (03/2008) (Fl)
France44SMn281.0762EN 10087 (09/1998) (FR)
France44SMn281.0762EN 10277-3 (03/2008) (FR)
Great Britain44SMn281.0762EN 10087 (09/1998) (GB)
Great Britain44SMn281.0762EN 10277-3 (03/2008) (GB)
Great Britain226 M 441.0762970 Part 1 (1996) withdrawn (GB)
Greece44SMn281.0762EN 10087 (09/1998) (GR)
Greece44SMn281.0762EN 10277-3 (03/2008) (GR)
Hungary44SMn281.0762EN 10087 (09/1998) (HU)
Hungary44SMn281.0762EN 10277-3 (03/2008) (HU)
Iceland44SMn281.0762EN 10087 (09/1998) (IS)
Iceland44SMn281.0762EN 10277-3 (03/2008) (IS)
India44C15S24~1.076214698 (1999) (IN)
Ireland44SMn281.0762EN 10087 (09/1998) (IE)
Ireland44SMn281.0762EN 10277-3 (03/2008) (IE)
ISO44SMn28~1.0762683-9 (1988) (ISO)
Italy44SMn281.0762EN 10087 (09/1998) (IT)
Italy44SMn281.0762EN 10277-3 (03/2008) (IT)
JapanSUM43~1.0762G 4804 (2008) (JP)
Latvia44SMn281.0762EN 10087 (09/1998) (LV)
Latvia44SMn281.0762EN 10277-3 (03/2008) (LV)
Lithuania44SMn281.0762EN 10087 (09/1998) (LT)
Lithuania44SMn281.0762EN 10277-3 (03/2008) (LT)
Luxemburg44SMn281.0762EN 10087 (09/1998) (LU)
Luxemburg44SMn281.0762EN 10277-3 (03/2008) (LU)
Malta44SMn281.0762EN 10087 (09/1998) (MT)
Malta44SMn281.0762EN 10277-3 (03/2008) (MT)
Netherlands44SMn281.0762EN 10087 (09/1998) (NL)
Netherlands44SMn281.0762EN 10277-3 (03/2008) (NL)
Norway44SMn281.0762EN 10087 (09/1998) (NO)
Norway44SMn281.0762EN 10277-3 (03/2008) (NO)
Poland44SMn281.0762EN 10087 (09/1998) (PL)
Poland44SMn281.0762EN 10277-3 (03/2008) (PL)
Portugal44SMn281.0762EN 10087 (09/1998) (PT)
Portugal44SMn281.0762EN 10277-3 (03/2008) (PT)
Republic of KoreaSUM 43~1.0762D 3567 (2002) (KR)
Romania44SMn281.0762EN 10087 (09/1998) (RO)
Romania44SMn281.0762EN 10277-3 (03/2008) (RO)
Serbia44SMn281.0762EN 10087 (09/1998) (CS)
Serbia44SMn281.0762EN 10277-3 (03/2008) (CS)
Slovak Republic44SMn281.0762EN 10087 (09/1998) (SK)
Slovak Republic44SMn281.0762EN 10277-3 (03/2008) (SK)
Slovenia44SMn281.0762EN 10087 (09/1998) (SL)
Slovenia44SMn281.0762EN 10277-3 (03/2008) (SL)
Spain44SMn281.0762EN 10087 (09/1998) (ES)
Spain44SMn281.0762EN 10277-3 (03/2008) (ES)
Sweden44SMn281.0762EN 10087 (09/1998) (SE)
Sweden44SMn281.0762EN 10277-3 (03/2008) (SE)
Switzerland44SMn281.0762EN 10087 (09/1998) (CH)
Switzerland44SMn281.0762EN 10277-3 (03/2008) (CH)
Turkey44SMn281.0762EN 10087 (09/1998) (TR)
Turkey44SMn281.0762EN 10277-3 (03/2008) (TR)
U.S.A.G11440 (UNS)~1.0762
U.S.A.1144 (AISI)~1.0762
U.S.A.A 29 (1144) (ASTM)~1.0762A 29-05(US)
U.S.A.A 108 (1144) (ASTM)~1.0762A 108-07(US)
U.S.A.A 311 (1144) (ASTM)~1.0762A 311-04(US)
U.S.A.A 510 (1144) (ASTM)~1.0762A 510-07/06(US)
U.S.A.A 519 (1144) (ASTM)~1.0762A 519-06(US)
U.S.A.A 521 (1144) (ASTM)~1.0762A 521-06(US)
U.S.A.A 576 (1144) (ASTM)~1.0762A 576-90 (06)(US)
U.S.A.A 711 (1144) (ASTM)~1.0762A 711-07(US)
U.S.A.1144 (SAE)~1.0762J 403 (2001) (US)

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey