AISI 4620 Low Alloy Steel

AISI 4620 Low Alloy Steel

AISI 4620 Steel Overview

AISI 4620 steel (UNS G46200) is a low alloy steel. This page lists the AISI 4620 material data sheets for 2 conditions: annealed, normalized. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.

Typical Uses of AISI 4620 Steel

General construction, general mechanical engineering, automotive, tools, axles, gears, springs.

AISI 4620 Steel Chemical Composition

C (carbon)0.17 – 0.22 %
Fe (iron)96.4 – 97.4 %
Mn (manganese)0.45 – 0.65 %
Mo (molybdenum)0.2 – 0.3 %
Ni (nickel)1.65 – 2 %
P (phosphorus)0 – 0.035 %
S (sulfur)0 – 0.04 %
Si (silicon)0.15 – 0.35 %

AISI 4620 Steel Material Data Sheets

AISI 4620 Annealed Material Data Sheet

AISI 4620 Normalized Material Data Sheet

AISI 4620 Steel Condition Comparison

See how yield strength, tensile strength and hardness change between conditions in the AISI 4620 Annealed vs Normalized: Yield, Tensile & Hardness Compared.

AISI 4620 Steel Parts from Turkey

Looking for AISI 4620 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 4620 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all low alloy steel grades.