AISI 1040 steel (UNS G10400) is a medium carbon steel. This page lists the AISI 1040 material data sheets for 13 conditions: annealed, as rolled, normalized, oil quenched & tempered at 205°C, oil quenched & tempered at 315°C, oil quenched & tempered at 425°C, oil quenched & tempered at 540°C, oil quenched & tempered at 650°C, water quenched & tempered at 205°C, water quenched & tempered at 315°C, water quenched & tempered at 425°C, water quenched & tempered at 540°C, water quenched & tempered at 650°C. Each data sheet covers designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing, durability and corrosion resistance.
Typical Uses of AISI 1040 Steel
Heavy duty shafts, axles, crankshafts, couplings, gears (if given a hardening treatment)
Looking for AISI 1040 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1040 steel parts in-house, heat treated to your specified condition, and inspects them before shipment. See all medium and high carbon steel grades.