Brass alloys are the most widely used group of copper alloys. Adding zinc to copper creates several different phases, which is why brasses cover such a broad range of properties.

Brass Strengths

Brass is economical, stands up well to many aggressive environments and is easy to fabricate and machine. It combines high electrical and thermal conductivity with useful strength, and it is available in a wide palette of colours, from red and orange to yellow, silver and white.

Brass Limitations

Brasses are not as strong as bronzes. They should not be specified for environments that cause dezincification, such as acidic or saline solutions.

Brass Designation

Brasses carry UNS numbers in the Cxxxxx format. Alpha brasses contain less than 36 wt% zinc, for example cap brass (5% Zn), gilding brass (15% Zn), cartridge brass (30% Zn) and yellow brass (34% Zn). Alpha-beta brasses contain more than 36 wt% zinc, such as Muntz metal (40% Zn).

Typical Uses of Brass Alloys

Valve and pump parts, taps and water pipes, fasteners, screws, bushings and bearings, springs, heat exchangers and condenser tubes, marine and automotive components, hot forgings, extrusions and deep-drawn parts, cartridge and shell casings, musical instruments, jewelry, architectural decoration, and door and window hardware.

Brass Compositional Summary

Copper with 5–40% zinc and varying additions of manganese, lead, iron and tin
Material familyMetal (non-ferrous)
Base materialCu (Copper)

Brass Microstructure

Up to about 36% zinc, brass forms the face-centred cubic alpha solid solution. Higher zinc contents produce the body-centred cubic beta phase, a second copper-zinc solid solution that orders into the beta-prime structure at room temperature. Above roughly 50% zinc the very brittle gamma phase appears. Alpha brasses typically show annealing twins.

Effect of Composition on Brass

More zinc raises strength and hardness at the expense of ductility and conductivity. Lead is added for better machinability, aluminium and tin raise strength and corrosion resistance, and silicon further improves corrosion resistance.

Brass Processing Properties

Feedstocks & Production

Brass mills are supplied with copper cakes or billets made from old cathodes, which serve as the starting material for brass production.

Forming

Brass forms very well and can be cast, drawn or spun.

Machining

Machinability is excellent.

Joining

Brass joins readily by most commercial methods, including riveting, soft soldering, silver brazing and friction welding.

Brass Grades

WROUGHT

CuZn10 (C22000) (Gilding Metal)

CuZn10, C22000, soft (gilding metal)

CuZn15 (C23000) (Red Brass)

CuZn15, C23000, soft (red brass)

CuZn20 (C24000) (Low Brass)

CuZn20, C24000, soft (low brass)

CuZn20Al2 (C68700) (Aluminum Brass)

CuZn20Al2, C68700, soft (aluminum brass)

CuZn27Al4.5 (High-Tensile Brass)

CuZn27Al4.5, as drawn (high-tensile brass)

CuZn28 (C25600) (Deep-Drawing/Cartridge Brass)

CuZn28, C25600, soft (deep-drawing/cartridge brass)

CuZn28Sn1 (C44300) (Admiralty Brass)

CuZn28Sn1, C44300, half hard (admiralty brass)
CuZn28Sn1, C44300, soft (admiralty brass)

CuZn30 (C26000) (Deep-Drawing/Cartridge Brass)

CuZn30, C26000, soft (deep-drawing/cartridge brass)

CuZn30 (C43600) (Arsenical 70/30 Brass)

CuZn30, C43600, hard (arsenical 70/30 brass)
CuZn30, C43600, soft (arsenical 70/30 brass)

CuZn33 (C26800) (Yellow Brass)

CuZn33, C26800, soft (yellow brass)

CuZn34Pb1 (C34000) (Leaded Clock Brass)

CuZn34Pb1, C34000, soft (leaded (clock) brass)

CuZn36 (C26800) (Basis Brass)

CuZn36, C26800, hard (basis brass)
CuZn36, C26800, soft (basis brass)

CuZn36Pb2 (C35300) (Leaded Clock Brass)

CuZn36Pb2, C35300, soft (leaded (clock) brass)

CuZn36Pb3 (C36000) (Free-Cutting Brass)

CuZn36Pb3, C36000, (cold worked), (free-cutting brass)
CuZn36Pb3, C36000, soft (free-cutting brass)

CuZn38Mn1.5 (High-Tensile Brass)

CuZn38Mn1.5, (hot worked), (high-tensile brass)
CuZn38Mn1.5, as drawn (high-tensile brass)

CuZn38Sn1 (C46400) (Naval Brass)

CuZn38Sn1, C46400, hard (naval brass)
CuZn38Sn1, C46400, soft (naval brass)

CuZn39Pb2 (C37700) (Leaded Clock Brass, Leaded Forging Brass)

CuZn39Pb2, C37700, (cold worked), (leaded (clock) brass)
CuZn39Pb2, C37700, (hot worked), (leaded (clock) brass)
CuZn39Pb2, C37700, (hot worked), (leaded (forging) brass)
CuZn39Pb2, C37700, soft (leaded (clock) brass)
CuZn39Pb2, C37700, soft (leaded (forging) brass)

CuZn40 (C28000) (Muntz Metal)

CuZn40, C28000, hard (muntz metal)
CuZn40, C28000, soft (muntz metal)

CuZn40Pb1 (C36500) (Leaded Muntz Metal)

CuZn40Pb1, C36500, (cold worked), (leaded muntz metal)
CuZn40Pb1, C36500, (hot worked), (leaded muntz metal)

CuZn40Pb3 (C37710) (Free-Cutting Brass)

CuZn40Pb3, C37710, (hot worked), (free-cutting brass)

CuZn5 (C21000) (Gilding Metal)

CuZn5, C21000, soft (gilding metal)

CAST

CuZn10Pb3Sn2 Cast

CuZn10Pb3Sn2, sand-cast

CuZn15As0.2 (C23000) (Brazable Brass)

CuZn15As0.2, C23000, sand-cast (brazable brass)

CuZn30Al5Mn4Fe2 Cast (High-Tensile Manganese Bronze)

CuZn30Al5Mn4Fe2, cast (high-tensile manganese bronze)

CuZn30Pb2 (C85400)

CuZn30Pb2, C85400, sand-cast

CuZn35Sn1 (C85700) (Naval Brass)

CuZn35Sn1, C85700, sand-cast (naval brass)

CuZn40 (C85500)

CuZn40, C85500, gravity die-cast

CuZn40Mn3Al2Fe2 (C86550) (High-Tensile Manganese Bronze)

CuZn40Mn3Al2Fe2, C86550, cast (high-tensile manganese bronze)

CuZn40Pb2 (C38000)

CuZn40Pb2, C38000, pressure die cast

CuZn40Pb2Sn1 (C85800) (Naval Brass)

CuZn40Pb2Sn1, C85800, gravity die-cast (naval brass)