Home » Brass Alloys » CuZn36Pb2 (C35300) Leaded Clock Brass, Soft Material Data Sheet
CuZn36Pb2 (C35300) Leaded Clock Brass Material Data Sheet (Wrought, Soft)
CuZn36Pb2 C35300 Soft Overview
CuZn36Pb2 C35300 soft is a wrought brass (UNS C35300), known as leaded clock brass. Condition: Soft. This CuZn36Pb2 C35300 soft material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for CuZn36Pb2 brass parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined CuZn36Pb2 brass parts in-house and inspects them before shipment.
CuZn36Pb2 Designation
CuZn36Pb2, wrought Condition Soft UNS number C35300 EN name CW606N ISO name CuZn37Pb2 JIS (Japanese) name C3530
CuZn36Pb2 Typical uses
Machined & blanked parts, spark plugs & battery terminals, dials & engraved plates.
CuZn36Pb2 C35300 Soft Composition detail
Cu (copper) 58.9 – 64.1 % Fe (iron) 0 – 0.1 % Pb (lead) 1.5 – 2.5 % Zn (zinc) 34.4 – 38.5 %
CuZn36Pb2 Physical properties
CuZn36Pb2 C35300 Soft Mechanical properties
Young’s modulus 98.9 – 105 GPa Specific stiffness 11.9 – 12.6 MN.m/kg Yield strength (elastic limit) 120 – 130 MPa Tensile strength 325 – 340 MPa Specific strength 14.4 – 15.7 kN.m/kg Elongation 40 – 45 % strain Compressive strength 120 – 130 MPa Flexural modulus 98.9 – 105 GPa Flexural strength (modulus of rupture) 120 – 130 MPa Shear modulus 36.6 – 38.9 GPa Bulk modulus 107 – 113 GPa Poisson’s ratio 0.34 – 0.35 Shape factor 29 Hardness – Vickers 59 – 72 HV Elastic stored energy (springs) 70.4 – 83.2 kJ/m3 Fatigue strength at 10^7 cycles 155 – 159 MPa Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles 149 – 165 MPa
CuZn36Pb2 Impact & fracture properties
Fracture toughness 67.9 – 70.4 MPa.m0.5 Toughness (G) 44.8 – 49.1 kJ/m2
CuZn36Pb2 C35300 Soft Thermal properties
Melting point 905 – 922 °C Maximum service temperature 180 – 190 °C Minimum service temperature -170 – -160 °C Thermal conductivity 121 – 129 W/m.°C Specific heat capacity 377 – 379 J/kg.°C Thermal expansion coefficient 19.1 – 20.3 µstrain/°C Thermal shock resistance 58.7 – 66 °C Thermal distortion resistance 6.07 – 6.63 MW/m Latent heat of fusion 220 – 240 kJ/kg
CuZn36Pb2 Electrical properties
Electrical resistivity 6.46 – 6.92 µohm.cm Electrical conductivity 24.9 – 26.7 %IACS Galvanic potential -0.34 – -0.26 V
CuZn36Pb2 Magnetic properties
Magnetic type Non-magnetic
CuZn36Pb2 Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 3450 – 3560 m/s Mechanical loss coefficient (tan delta) 2.37e-4 – 2.78e-4
CuZn36Pb2 Processing properties
Metal casting Unsuitable Metal cold forming Excellent Metal hot forming Excellent Metal press forming Excellent Metal deep drawing Limited use Machining speed 88.4 m/min Weldability Notes: Preheating and post weld heat treatments are required, and contains hazardous elements Poor
CuZn36Pb2 Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Acceptable Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oxidation at 500C Limited use UV radiation (sunlight) Excellent Galling resistance (adhesive wear) Excellent Flammability Non-flammable
CuZn36Pb2 C35300 Soft Corrosion resistance
Stress corrosion cracking Note: Rated in ammoniacal; Other susceptible environments: Water, amine, dinitrogen tetroxide Highly susceptible
CuZn36Pb2 Notes
CuZn36Pb2 C35300 Soft Other notes (s)=soft; (1/2 h)=half hard; (h)=hard; (xh)=extra hard; (hr) = hot rolled; (w)=soln heat-trtd; (wh)=soln heat-trtd & work hdnd; (wp)=soln heat-trtd & precip hdnd; (whp)=precip hdnd after cold-wkng; (wph)=work hdnd after precip hdng.
CuZn36Pb2 Standards with similar compositions
Australia: 353 to AS 1567, C35300 to AS 2738Canada: HC.4.ZP352 to CSA HC.4.3France: CuZn35Pb2 to NF A51-105International: CuZn35Pb2 to ISO 1634, CuZn35Pb2 to ISO 1637, CuZn35Pb2 to ISO 1638, CuZn35Pb2 to ISO 426-2UK: CZ119 to BS 2870, CZ119 to BS 2871, CZ119 to BS 2873, CZ119 to BS 2874USA: C35300, C35300 to ASTM B121/B121M, C35300 to ASTM B453M, C35300 to CDA Datasheet, UNS C35300Tradenames: 3530, ANSONIA ALLOY C35300, BOHNALLOY R63, BOOTH B76, BOSCH (ME-16), BRIDGEPORT NO. 62, CLOCK BRASS-243, DELTA TR1 GENERAL PURPOSE ROD AND BAR, DELTA TR1 HIGH SPEED MACHINING ROD, HIGH LEADED BRASS 353, HIGH LEADED BRASS 3531, HIGH LEADED BRASS 62, HIGH LEADED BRASS 62%, HOOKER BRASS, IMI 433, LEADED FLANGING BRASS, LEDRITE 2, MCKECHNIE 20, MESSING 63PB, MUELLER 3450, NITTANY NO. 2, NITTANY NO. 38, OLIN HIGH LEADED BRASS 353, PRYM 263, RM 433, WESTERN ALLOY NO. 68, WESTERN HIGH LEADED BRASS #68, WIELAND-Z14, WIELAND-Z21