EN numerical alloy designationEN symbolic alloy designationCorresponding ISO alloy designationCorresponding AA alloy designationCorresponding JIS alloy designation
EN AC-21000EN AC-AlCu4MgTiAl Cu4MgTi204.0AC1B
EN AC-21100EN AC-Al Cu4TiAl Cu4Ti–Al-Cu4Ti
EN AC-21200EN AC-Al Cu5MnMg–––
EN AC-41000EN AC-Al Si2MgTiAl Si2MgTi––
EN AC-42000EN AC-AlSi7MgAl Si7Mg356.0AC4C
EN AC-42100EN AC-Al Si7Mg0.3Al Si7Mg0.3A356.0AC4CH
EN AC-42200EN AC-AlSi7Mg0.6Al Si7Mg0.6357.0–
EN AC-43000EN AC-Al Si10Mg(a)Al Si10Mg–AC4A.Al-Si10Mg
EN AC-43100EN AC-Al Si10Mg(b)Al Si10Mg–AC4A.Al-Si10Mg
EN AC-43200EN AC-Al Si10Mg(Cu)Al Si10Mg(Cu)––
EN AC-43300EN AC-Al Si9MgAl Si9Mg––
EN AC-43400EN AC-Al Si10Mg(Fe)Al Si10Mg(Fe)–ADC3
EN AC-43500EN AC-Al Si10MnMg–365.0–
EN AC-44000EN AC-Al Si11Al Si11––
EN AC-44100EN AC-Al Si12(b)Al Si12(b)B413.0AC3A.Al-Si12
EN AC-44200EN AC-Al Si12(a)Al Si12(a)––
EN AC-44300EN AC-Al Si12(Fe)(a)Al Si12(Fe)A413.0ADC1
EN AC-44400EN AC-Al Si9Al Si9––
EN AC-44500EN AC-Al Si12(Fe)(b)–––
EN AC-45000EN AC-Al Si6Cu4Al Si6Cu4–Al-Si6Cu4
EN AC-45100EN AC-Al Si5Cu3MgAl Si5Cu3Mg363.0–
EN AC-45300EN AC-Al Si5Cu1MgAl Si5Cu1Mg355.0AC40
EN AC-45400EN AC-Al Si5Cu3Al Si5Cu3–Al-Si5Cu3
EN AC-45500EN AC-Al Si7Cu0.5Mg–––
EN AC-46000EN AC-Al Si9Cu3(Fe)Al Si9Cu3(Fe)–ADC10
EN AC-46100EN AC-Al Si11Cu2(Fe)Al Si11Cu2(Fe)–ADC12Z
EN AC-46200EN AC-Al Si8Cu3Al Si8Cu3380.0AC4B
EN AC-46300EN AC-Al Si7Cu3MgAl Si7Cu3Mg320.0–
EN AC-46400EN AC-Al Si9Cu1MgAl Si9Cu1Mg––
EN AC-46500EN AC-Al Si9Cu3(Fe)(Zn)Al Si9Cu3(Fe) (Zn)–ADC10Z
EN AC-46600EN AC-Al Si7Cu2Al Si7Cu2––
EN AC-47000EN AC-Al Si12(Cu)Al Si12(Cu)–Al-Si12Cu
EN AC-47100EN AC-Al Si12Cu1(Fe)Al Si12Cu1(Fe)––
EN AC-48000EN AC-Al
Si12CuNiMg
Al Si12CuNiMg–AC8A
EN AC-48100EN AC-Al Si17Cu4MgAl Si17Cu4Mg8390.0ADC14
EN AC 51100EN AC-Al Mg3–––
EN AC-51200EN AC-Al Mg9Al Mg9518.0Al-Mg10
EN AC-51300EN AC-Al Mg5Al Mg5–ADC5, AC7A, Al-Mg6
EN AC-51400EN AC-Al Mg5(Si)Al Mg5(Si)–Al-Mg5Si1
EN AC-51500EN AC-Al Mg5Si2Mn–––
EN AC-71100EN AC-Al Zn10Si8MgAl Zn 10Si8Mg––

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey