Brass Alloys
Brass Alloys Overview
| Brass alloys are the most widely used group of copper alloys. Adding zinc to copper creates several different phases, which is why brasses cover such a broad range of properties. |
Brass Strengths
| Brass is economical, stands up well to many aggressive environments and is easy to fabricate and machine. It combines high electrical and thermal conductivity with useful strength, and it is available in a wide palette of colours, from red and orange to yellow, silver and white. |
Brass Limitations
| Brasses are not as strong as bronzes. They should not be specified for environments that cause dezincification, such as acidic or saline solutions. |
Brass Designation
| Brasses carry UNS numbers in the Cxxxxx format. Alpha brasses contain less than 36 wt% zinc, for example cap brass (5% Zn), gilding brass (15% Zn), cartridge brass (30% Zn) and yellow brass (34% Zn). Alpha-beta brasses contain more than 36 wt% zinc, such as Muntz metal (40% Zn). |
Typical Uses of Brass Alloys
| Valve and pump parts, taps and water pipes, fasteners, screws, bushings and bearings, springs, heat exchangers and condenser tubes, marine and automotive components, hot forgings, extrusions and deep-drawn parts, cartridge and shell casings, musical instruments, jewelry, architectural decoration, and door and window hardware. |
Brass Compositional Summary
| Copper with 5–40% zinc and varying additions of manganese, lead, iron and tin | |
| Material family | Metal (non-ferrous) |
| Base material | Cu (Copper) |
Brass Microstructure
| Up to about 36% zinc, brass forms the face-centred cubic alpha solid solution. Higher zinc contents produce the body-centred cubic beta phase, a second copper-zinc solid solution that orders into the beta-prime structure at room temperature. Above roughly 50% zinc the very brittle gamma phase appears. Alpha brasses typically show annealing twins. |
Effect of Composition on Brass
| More zinc raises strength and hardness at the expense of ductility and conductivity. Lead is added for better machinability, aluminium and tin raise strength and corrosion resistance, and silicon further improves corrosion resistance. |
Brass Processing Properties
Feedstocks & Production
| Brass mills are supplied with copper cakes or billets made from old cathodes, which serve as the starting material for brass production. |
Forming
| Brass forms very well and can be cast, drawn or spun. |
Machining
| Machinability is excellent. |
Joining
| Brass joins readily by most commercial methods, including riveting, soft soldering, silver brazing and friction welding. |