CuZn40Pb2Sn1 C85800 Gravity Die-Cast Overview
CuZn40Pb2Sn1 C85800 gravity die-cast is a cast brass (UNS C85800), known as naval brass. Condition: Gravity Die-Cast. This CuZn40Pb2Sn1 C85800 gravity die-cast material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for CuZn40Pb2Sn1 brass castings from Turkey (Türkiye)? Modulus Metal supplies CuZn40Pb2Sn1 brass castings with in-house CNC machining and inspects them before shipment.
CuZn40Pb2Sn1 Designation
CuZn40Pb2Sn1 UNS number C85800 ISO name CuZn35Pb1Sn1
CuZn40Pb2Sn1 Typical uses
Accurate general-purpose castings, food & pickling plant especially when machined.
CuZn40Pb2Sn1 C85800 Gravity Die-Cast Composition detail
Al (aluminum) 0 – 0.5 % As (arsenic) 0 – 0.05 % Cu (copper) 57 – 66 % Fe (iron) 0 – 0.5 % Mn (manganese) 0 – 0.25 % Ni (nickel) 0 – 0.5 % P (phosphorus) 0 – 0.01 % Pb (lead) 0 – 1.5 % S (sulfur) 0 – 0.05 % Sb (antimony) 0 – 0.05 % Si (silicon) 0 – 0.25 % Sn (tin) 0 – 1.5 % Zn (zinc) 31 – 41 %
CuZn40Pb2Sn1 Physical properties
CuZn40Pb2Sn1 C85800 Gravity Die-Cast Mechanical properties
Young’s modulus 91.1 – 92.9 GPa Specific stiffness 11.3 – 11.7 MN.m/kg Yield strength (elastic limit) 200 – 220 MPa Tensile strength 360 – 400 MPa Specific strength 25 – 27.5 kN.m/kg Elongation 10 – 20 % strain Compressive strength 90 – 120 MPa Flexural modulus 91.1 – 92.9 GPa Flexural strength (modulus of rupture) 90 – 120 MPa Shear modulus 33.7 – 34.4 GPa Bulk modulus 98.4 – 100 GPa Poisson’s ratio 0.34 – 0.35 Shape factor 26 Hardness – Vickers 60 – 70 HV Elastic stored energy (springs) 218 – 263 kJ/m3 Fatigue strength at 10^7 cycles 147 – 159 MPa Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles 135 – 173 MPa
CuZn40Pb2Sn1 Impact & fracture properties
Fracture toughness 70.4 – 79.2 MPa.m0.5 Toughness (G) 54 – 68 kJ/m2
CuZn40Pb2Sn1 C85800 Gravity Die-Cast Thermal properties
Melting point 882 – 902 °C Maximum service temperature 120 – 130 °C Minimum service temperature -273 °C Thermal conductivity 80.5 – 87.3 W/m.°C Specific heat capacity 373 – 375 J/kg.°C Thermal expansion coefficient 20.1 – 20.5 µstrain/°C Thermal shock resistance 107 – 118 °C Thermal distortion resistance 3.96 – 4.31 MW/m Latent heat of fusion 220 – 240 kJ/kg
CuZn40Pb2Sn1 Electrical properties
Electrical resistivity 8.4 – 8.8 µohm.cm Electrical conductivity 19.6 – 20.5 %IACS Galvanic potential -0.33 – -0.25 V
CuZn40Pb2Sn1 Magnetic properties
Magnetic type Non-magnetic
CuZn40Pb2Sn1 Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 3370 – 3420 m/s Mechanical loss coefficient (tan delta) 2.78e-4 – 4.94e-4
CuZn40Pb2Sn1 Processing properties
Metal casting Acceptable Metal cold forming Unsuitable Metal hot forming Unsuitable Metal press forming Unsuitable Metal deep drawing Unsuitable Machining speed 97.5 m/min Weldability Notes: Preheating and post weld heat treatments are required, and contains hazardous elements Poor
CuZn40Pb2Sn1 Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Acceptable Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oxidation at 500C Limited use UV radiation (sunlight) Excellent Galling resistance (adhesive wear) Excellent Flammability Non-flammable
CuZn40Pb2Sn1 C85800 Gravity Die-Cast Corrosion resistance
Stress corrosion cracking Note: Rated in ammoniacal; Other susceptible environments: Water, amine, dinitrogen tetroxide Highly susceptible
CuZn40Pb2Sn1 Notes
CuZn40Pb2Sn1 C85800 Gravity Die-Cast Other notes (s)=soft; (1/2 h)=half hard; (h)=hard; (xh)=extra hard; (hr) = hot rolled; (w)=soln heat-trtd; (wh)=soln heat-trtd & work hdnd; (wp)=soln heat-trtd & precip hdnd; (whp)=precip hdnd after cold-wkng; (wph)=work hdnd after precip hdng.
CuZn40Pb2Sn1 Standards with similar compositions
USA: C85800, C85800 to ASTM B30, UNS C85800Tradenames: KRAMER DIE CAST YELLOW BRASS, M AND A NO. 18, PRESSURE DIE CASTING, PROMET 406, TECHNI-CAST YB2, TYB-2