CuZn40Pb1 (C36500) Leaded Muntz Metal, Hot Worked Material Data Sheet

CuZn40Pb1 (C36500) Leaded Muntz Metal Material Data Sheet (Wrought, Hot Worked)

CuZn40Pb1 C36500 Hot Worked Overview

CuZn40Pb1 C36500 hot worked is a wrought brass (UNS C36500), known as leaded muntz metal. Condition: Hot worked. This CuZn40Pb1 C36500 hot worked material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for CuZn40Pb1 brass parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined CuZn40Pb1 brass parts in-house and inspects them before shipment.

CuZn40Pb1 Designation

CuZn40Pb1, wrought
ConditionHot worked
UNS numberC36500
EN nameCW610N
ISO nameCuZn40Pb
GB (Chinese) nameHPb61-1

CuZn40Pb1 Typical uses

Condenser tube plates, porthole casings, extrusions, hot forgings, decorative brassware.

CuZn40Pb1 C36500 Hot Worked Composition detail

Cu (copper)57.1–61.8%
Fe (iron)0–0.15%
Pb (lead)0.25–0.7%
Sn (tin)0–0.25%
Zn (zinc)37.9–41.8%

CuZn40Pb1 Physical properties

Density8.18–8.35g/cm3

CuZn40Pb1 C36500 Hot Worked Mechanical properties

Young’s modulus97–103GPa
Specific stiffness11.7–12.5MN.m/kg
Yield strength (elastic limit)160–170MPa
Tensile strength380–390MPa
Specific strength19.3–20.6kN.m/kg
Elongation30–40% strain
Compressive strength160–170MPa
Flexural modulus97–103GPa
Flexural strength (modulus of rupture)160–170MPa
Shear modulus35.9–38.1GPa
Bulk modulus105–111GPa
Poisson’s ratio0.34–0.35 
Shape factor28
Hardness – Vickers80–100HV
Elastic stored energy (springs)127–145kJ/m3
Fatigue strength at 10^7 cycles171–174MPa
Fatigue strength model (stress range)
Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
163–183MPa

CuZn40Pb1 Impact & fracture properties

Fracture toughness59.4–61.3MPa.m0.5
Toughness (G)34.9–38kJ/m2

CuZn40Pb1 C36500 Hot Worked Thermal properties

Melting point882–902°C
Maximum service temperature97–110°C
Minimum service temperature-273  °C
Thermal conductivity120–128W/m.°C
Specific heat capacity376–378J/kg.°C
Thermal expansion coefficient19.4–20.6µstrain/°C
Thermal shock resistance78.4–86.9°C
Thermal distortion resistance5.93–6.48MW/m
Latent heat of fusion220–240kJ/kg

CuZn40Pb1 Electrical properties

Electrical resistivity6.17–6.61µohm.cm
Electrical conductivity26.1–27.9%IACS
Galvanic potential-0.35–-0.27V

CuZn40Pb1 Magnetic properties

Magnetic typeNon-magnetic

CuZn40Pb1 Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity3420–3530m/s
Mechanical loss coefficient (tan delta)1.38e-4–1.56e-4 

CuZn40Pb1 Processing properties

Metal castingUnsuitable
Metal cold formingAcceptable
Metal hot formingExcellent
Metal press formingAcceptable
Metal deep drawingLimited use
Machining speed73.2 m/min
Weldability
Notes: Preheating and post weld heat treatments are required, and contains hazardous elements
Poor

CuZn40Pb1 Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsAcceptable
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oxidation at 500CLimited use
UV radiation (sunlight)Excellent
Galling resistance (adhesive wear)Excellent
FlammabilityNon-flammable

CuZn40Pb1 C36500 Hot Worked Corrosion resistance

Stress corrosion cracking
Note: Rated in ammoniacal; Other susceptible environments: Water, amine, dinitrogen tetroxide
Highly susceptible

CuZn40Pb1 Notes

CuZn40Pb1 C36500 Hot Worked Other notes
(s)=soft; (1/2 h)=half hard; (h)=hard; (xh)=extra hard; (hr) = hot rolled; (w)=soln heat-trtd; (wh)=soln heat-trtd & work hdnd; (wp)=soln heat-trtd & precip hdnd; (whp)=precip hdnd after cold-wkng; (wph)=work hdnd after precip hdng.

CuZn40Pb1 Standards with similar compositions

Australia: 365 to AS 1567, 365 to AS 1568, C36500 to AS 2738
Canada: HC.4.ZP391(365) to CSA
Denmark: 5163 to DS 3003
Europe: CW610N to CEN EN 12164, CW610N to CEN EN 12165, CW610N to CEN EN 12166, CW610N to CEN EN 12167, CW610N to CEN EN 12420, CW610N to CEN EN 1652, CW610N to CEN EN 1653
Finland: CuZn40Pb to SFS 2925
International: CuZn40Pb to ISO 1634, CuZn40Pb to ISO 1637, CuZn40Pb to ISO 1638, CuZn40Pb to ISO 426-2
Norway: 16140 to NS 16140
Sweden: 5163-00 to SIS 145163, 5163-04 to SIS 145163
UK: CZ123 to BS 2870, CZ123 to BS 2872, CZ123 to BS 2875
USA: C36500, C36500 to ASTM B124M, C36500 to ASTM B171/B171M, C36500 to ASTM B283, UNS C36500, UNS C36600
Tradenames: FUCHS 2360, LEADED MUNTZ METAL, LEADED MUNTZ METAL-365, MCKECHNIE SS1, REVERE ALLOY NO. 365