CuZn39Pb2 C37700 soft leaded clock brass is a wrought brass (UNS C37700), known as leaded clock brass. Condition: Soft. This CuZn39Pb2 C37700 soft leaded clock brass material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for CuZn39Pb2 brass parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined CuZn39Pb2 brass parts in-house and inspects them before shipment.
Stress corrosion cracking Note: Rated in ammoniacal; Other susceptible environments: Water, amine, dinitrogen tetroxide
Highly susceptible
CuZn39Pb2 Notes
CuZn39Pb2 C37700 Soft (Leaded Clock Brass) Other notes
(s)=soft; (1/2 h)=half hard; (h)=hard; (xh)=extra hard; (hr) = hot rolled; (w)=soln heat-trtd; (wh)=soln heat-trtd & work hdnd; (wp)=soln heat-trtd & precip hdnd; (whp)=precip hdnd after cold-wkng; (wph)=work hdnd after precip hdng.
CuZn39Pb2 Standards with similar compositions
Denmark: 5167 to DS 3003
France: CuZn38Pb2 to NF A51-101, CuZn39Pb2 to NF A51-101
Germany: 2.038 to DIN, CuZn39Pb2 to DIN
International: CuZn38Pb2 to ISO 1634, CuZn38Pb2 to ISO 1635, CuZn38Pb2 to ISO 1637, CuZn38Pb2 to ISO 1638, CuZn38Pb2 to ISO 426-2
Japan: C3561 P/R to JIS H3100
Norway: 16135 to NS 16135
UK: CZ120 to BS 2870
USA: 60Cu-2.0Pb-37.5Zn to AMS 4614, 60Cu-38Zn-2Pb to MIL C-13351, 60Cu-38Zn-2Pb to QQ B-626, C37700, C37700 to ASTM B124M, C37700 to ASTM B283, C37700 to SAE J463, UNS C37700