PA66 (nylon 66) is the strongest aliphatic polyamide. It is tougher at low temperature than POM or PBT, resists abrasion better and absorbs less water than PA6, covers the widest service temperature range of the polyamides and has the lowest permeability to petrol, mineral oil and fluorocarbon refrigerants. Its cost is low, similar to PA6.
PA66 Limitations
Water absorption is high compared with some grades, and dry impact strength and elongation are lower than in some other polyamides. It has the weakest UV and oxidation resistance of the family and resists weak acids less well than some grades.
PA66 Designation
PA66, also written 6.6 or 6/6.
PA66 Compositional Summary
(NH-(CH2)6-NH-CO-(CH2)4-CO)n
Material family
Plastic (thermoplastic, semi-crystalline)
Base material
PA66 (Polyamide / nylon 66)
CAS number
32131-17-2
PA66 Notes
In many applications nylon 6 and nylon 66 are interchangeable, and the choice often comes down to local availability.
PA66 Processing Properties
Feedstocks and Production
Made from hexamethylene diamine and adipic acid.
Surface Treatment
Only some grades can be plated.
PA66 Parts from Turkey
Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.