Home » PA (Polyamide / Nylon) » PA66 (Polyamide 66 / Nylon 66) » PA66 Unfilled Grades » PA66 Flame Retarded Grade Material Data Sheet
PA66 Flame Retarded Grade (Polyamide 66) Material Data Sheet
PA66 Flame Retarded Grade Overview
PA66 flame retarded grade is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, Unreinforced, Flame Retarded). This PA66 flame retarded grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.
PA66 Flame Retarded Grade Designation
Polyamide (Nylon) (Type 66, Unreinforced, Flame Retarded) Tradenames Addinyl, Adell, Ashlene, Durethan, Frianyl, Hyundai, Kopa, Leona, Nyloy, Plustek, Radiflam, Starflam, Technyl, Vitamide, Wellamid, Zytel
PA66 Flame Retarded Grade Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA66 Flame Retarded Grade Composition detail
Polymer 85 – 95 % Flame retardant 5 – 15 %
PA66 Flame Retarded Grade Physical properties
PA66 Flame Retarded Grade Mechanical properties
Young’s modulus 1.63 – 2.04 GPa Specific stiffness 1.4 – 1.76 MN.m/kg Yield strength (elastic limit) 48.7 – 60.7 MPa Tensile strength 40.5 – 49.5 MPa Specific strength 42 – 52.3 kN.m/kg Elongation 19.9 – 28.7 % strain Elongation at yield 12.9 – 24.5 % strain Compressive modulus 1.74 – 1.93 GPa Compressive strength 51.3 – 56.7 MPa Flexural modulus 1.37 – 1.64 GPa Flexural strength (modulus of rupture) 47.7 – 58.3 MPa Shear modulus 0.638 – 0.671 GPa Shear strength 24.3 – 29.7 MPa Bulk modulus 2.93 – 3.24 GPa Poisson’s ratio 0.386 – 0.401 Shape factor 4.3 Hardness – Vickers 16 – 17 HV Hardness – Rockwell M 94 – 104 Hardness – Rockwell R 94 – 104 Hardness – Brinell 62 – 78 HB Hardness – Shore D 75 – 78 Elastic stored energy (springs) 643 – 1020 kJ/m3 Fatigue strength at 10^7 cycles 17.1 – 18.9 MPa
PA66 Flame Retarded Grade Impact & fracture properties
Fracture toughness 3.46 – 3.82 MPa.m0.5 Toughness (G) 6.27 – 8.38 kJ/m2 Impact strength, notched 23 °C 3.7 – 5.9 kJ/m2 Impact strength, notched -30 °C 1.32 – 2.88 kJ/m2 Impact strength, unnotched 23 °C 53.4 – 96.1 kJ/m2
PA66 Flame Retarded Grade Thermal properties
Melting point 249 – 265 °C Glass temperature 54 – 66 °C Heat deflection temperature 0.45MPa 210 – 213 °C Heat deflection temperature 1.8MPa 77 – 93 °C Maximum service temperature 90 – 130 °C Minimum service temperature -81 – -71 °C Thermal conductivity 0.291 – 0.302 W/m.°C Specific heat capacity 1430 – 1480 J/kg.°C Thermal expansion coefficient 79.2 – 80.8 µstrain/°C Thermal shock resistance 319 – 435 °C Thermal distortion resistance 0.00363 – 0.00379 MW/m
PA66 Flame Retarded Grade Electrical properties
Electrical resistivity 5.28e19 – 1.32e21 µohm.cm Electrical conductivity 1.31e-19 – 3.27e-18 %IACS Dielectric constant (relative permittivity) 5.23 – 7.37 Dissipation factor (dielectric loss tangent) 0.0257 – 0.0677 Dielectric strength (dielectric breakdown) 41.3 – 70.2 MV/m Comparative tracking index 350 – 600 V
PA66 Flame Retarded Grade Magnetic properties
Magnetic type Non-magnetic
PA66 Flame Retarded Grade Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 1180 – 1330 m/s Mechanical loss coefficient (tan delta) 0.0205 – 0.0227
PA66 Flame Retarded Grade Absorption & permeability
Water absorption @ 24 hrs 0.59 – 0.96 % Water absorption @ sat 6.6 – 8.7 % Humidity absorption @ sat 1.7 – 2.3 % Water vapor transmission 0.865 – 1.46 g.mm/m².day Permeability (O2) 0.339 – 0.995 cm³.mm/m².day.atm
PA66 Flame Retarded Grade Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 1 – 1.6 % Melt temperature 212 – 293 °C Mold temperature 40 – 60 °C Molding pressure range 6.88 – 103 MPa
PA66 Flame Retarded Grade Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Poor Flammability Self-extinguishing