PA66 50% Glass Fiber Material Data Sheet

PA66 50% Glass Fiber (Polyamide 66) Material Data Sheet

PA66 50% Glass Fiber Overview

PA66 50% glass fiber is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 50% Glass Fiber). This PA66 50% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.

PA66 50% Glass Fiber Designation

Polyamide (Nylon) (Type 66, 50% Glass Fiber)
TradenamesAkromid, Altech, Aquaforce, Ashlene, Badamid, Bergamid, Celstran, Compamid, Durethan, Edgetek, Latamid, Leona, LNP Thermocomp, Niretan, Nylaforce, Nypol, Pentamid, Plustek, Polybest, Polytron, Radilon, Scanamid, Schulamid, Slovamid, Staramide, Strator, Technyl, Tecomid, Terez, Tislamid, Torzen, Ultramid, Vitamide, Wellamid

PA66 50% Glass Fiber Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA66 50% Glass Fiber Composition detail

Polymer50  %
Glass (fiber)50  %

PA66 50% Glass Fiber Physical properties

Density1.56–1.59g/cm3

PA66 50% Glass Fiber Mechanical properties

Young’s modulus10.9–13.6GPa
Specific stiffness6.92–8.64MN.m/kg
Yield strength (elastic limit)156–194MPa
Tensile strength159–194MPa
Specific strength99–123kN.m/kg
Elongation2.62–3.78% strain
Elongation at yield2.21–4.19% strain
Compressive modulus11.6–12.8GPa
Compressive strength201–222MPa
Flexural modulus9.1–10.9GPa
Flexural strength (modulus of rupture)225–275MPa
Shear modulus4.44–4.66GPa
Shear strength95.3–117MPa
Bulk modulus12.3–13.6GPa
Poisson’s ratio0.329–0.343 
Shape factor6.5
Hardness – Vickers50–55HV
Hardness – Rockwell M184–204 
Hardness – Rockwell R184–204 
Hardness – Brinell117–147HB
Hardness – Shore D98–102 
Elastic stored energy (springs)988–1560kJ/m3
Fatigue strength at 10^7 cycles67.1–74.1MPa

PA66 50% Glass Fiber Impact & fracture properties

Fracture toughness5.07–5.61MPa.m0.5
Toughness (G)2.02–2.7kJ/m2
Impact strength, notched 23 °C17.5–34kJ/m2
Impact strength, notched -30 °C13.4–29.2kJ/m2
Impact strength, unnotched 23 °C83.4–123kJ/m2
Impact strength, unnotched -30 °C75.7–113kJ/m2

PA66 50% Glass Fiber Thermal properties

Melting point250–271°C
Glass temperature54–66°C
Heat deflection temperature 0.45MPa225–276°C
Heat deflection temperature 1.8MPa225–276°C
Maximum service temperature90–130°C
Minimum service temperature-81–-71°C
Thermal conductivity0.586–0.61W/m.°C
Specific heat capacity1280–1330J/kg.°C
Thermal expansion coefficient58.3–60.7µstrain/°C
Thermal shock resistance206–280°C
Thermal distortion resistance0.00978–0.0103MW/m

PA66 50% Glass Fiber Electrical properties

Electrical resistivity2.23e19–5.57e20µohm.cm
Electrical conductivity3.1e-19–7.73e-18%IACS
Dielectric constant (relative permittivity)9.63–13.6 
Dissipation factor (dielectric loss tangent)0.101–0.265 
Dielectric strength (dielectric breakdown)35.8–60.9MV/m
Comparative tracking index450–550V

PA66 50% Glass Fiber Magnetic properties

Magnetic typeNon-magnetic

PA66 50% Glass Fiber Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2630–2940m/s
Mechanical loss coefficient (tan delta)0.00795–0.00878 

PA66 50% Glass Fiber Absorption & permeability

Water absorption @ 24 hrs0.46–0.74%
Water absorption @ sat3.8–5%
Humidity absorption @ sat1.1–1.4%

PA66 50% Glass Fiber Processing properties

Polymer injection moldingLimited use
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.091 – 0.11 %
Melt temperature235 – 310 °C
Mold temperature40 – 60 °C
Molding pressure range68.8 – 138 MPa

PA66 50% Glass Fiber Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Poor
FlammabilitySlow-burning