PA66 5% Stainless Steel Long Fiber Material Data Sheet

PA66 5% Stainless Steel Long Fiber (Polyamide 66) Material Data Sheet

PA66 5% Stainless Steel Long Fiber Overview

PA66 5% stainless steel long fiber is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 5-6% Stainless Steel Long Fiber, Conductive – EMI Shielding). This PA66 5% stainless steel long fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.

PA66 5% Stainless Steel Long Fiber Designation

Polyamide (Nylon) (Type 66, 5-6% Stainless Steel Long Fiber, Conductive – EMI Shielding)
TradenamesCelstran

PA66 5% Stainless Steel Long Fiber Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA66 5% Stainless Steel Long Fiber Composition detail

Polymer94–95%
Stainless steel (fiber)5–6%

PA66 5% Stainless Steel Long Fiber Physical properties

Density1.18–1.2g/cm3

PA66 5% Stainless Steel Long Fiber Mechanical properties

Young’s modulus1.53–1.91GPa
Specific stiffness1.29–1.61MN.m/kg
Yield strength (elastic limit)40–49.9MPa
Tensile strength48.6–59.4MPa
Specific strength33.6–41.9kN.m/kg
Elongation5.54–7.98% strain
Elongation at yield4.43–8.41% strain
Compressive modulus1.63–1.8GPa
Compressive strength61.5–68MPa
Flexural modulus1.34–1.61GPa
Flexural strength (modulus of rupture)60.8–74.4MPa
Shear modulus0.598–0.629GPa
Shear strength29.1–35.6MPa
Bulk modulus2.72–3GPa
Poisson’s ratio0.384–0.4 
Shape factor4.61
Hardness – Vickers13–14HV
Hardness – Rockwell M104–115 
Hardness – Rockwell R104–115 
Hardness – Shore D78–82 
Elastic stored energy (springs)463–737kJ/m3
Fatigue strength at 10^7 cycles20.5–22.7MPa

PA66 5% Stainless Steel Long Fiber Impact & fracture properties

Fracture toughness3.41–3.77MPa.m0.5
Toughness (G)6.51–8.69kJ/m2
Impact strength, notched 23 °C4.49–8.72kJ/m2
Impact strength, notched -30 °C3.19–6.93kJ/m2

PA66 5% Stainless Steel Long Fiber Thermal properties

Melting point260–265°C
Glass temperature54–66°C
Heat deflection temperature 0.45MPa126–167°C
Heat deflection temperature 1.8MPa121–161°C
Maximum service temperature90–130°C
Minimum service temperature-81–-71°C
Thermal conductivity0.293–0.304W/m.°C
Specific heat capacity1470–1530J/kg.°C
Thermal expansion coefficient96–97.9µstrain/°C
Thermal shock resistance231–314°C
Thermal distortion resistance0.00301–0.00315MW/m

PA66 5% Stainless Steel Long Fiber Electrical properties

Electrical resistivity10000–1e6µohm.cm
Electrical conductivity1.72e-4–0.0172%IACS
Galvanic potential-0.14–-0.06V

PA66 5% Stainless Steel Long Fiber Magnetic properties

Magnetic typeMagnetic

PA66 5% Stainless Steel Long Fiber Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity1130–1270m/s
Mechanical loss coefficient (tan delta)0.0207–0.0229 

PA66 5% Stainless Steel Long Fiber Absorption & permeability

Water absorption @ 24 hrs0.58–0.95%
Water absorption @ sat6.7–8.9%
Humidity absorption @ sat1.9–2.6%

PA66 5% Stainless Steel Long Fiber Processing properties

Polymer injection moldingLimited use
Polymer extrusionUnsuitable
Polymer thermoformingLimited use
Linear mold shrinkage0.364 – 0.44 %
Melt temperature223 – 299 °C
Molding pressure range68.8 – 138 MPa

PA66 5% Stainless Steel Long Fiber Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Poor
FlammabilitySlow-burning