PA66 40% Glass and Mineral Material Data Sheet

PA66 40% Glass and Mineral (Polyamide 66) Material Data Sheet

PA66 40% Glass and Mineral Overview

PA66 40% glass and mineral is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 40% Glass and Mineral). This PA66 40% glass and mineral material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.

PA66 40% Glass and Mineral Designation

Polyamide (Nylon) (Type 66, 40% Glass and Mineral)
TradenamesAkulon, Alcom, Bestnyl, Chemlon, Clariant, Durethan, Ecolon, Hifill, Hylon, Kepamid, Maxamid, Minlon, Nybex, Scanamid, Schulamid, Technyl, Tekamid, Ultramid, Wellamid

PA66 40% Glass and Mineral Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA66 40% Glass and Mineral Composition detail

Polymer60  %
Glass (fiber)15–25%
Mineral (unspecified)15–25%

PA66 40% Glass and Mineral Physical properties

Density1.45–1.48g/cm3

PA66 40% Glass and Mineral Mechanical properties

Young’s modulus5.11–6.38GPa
Specific stiffness3.49–4.36MN.m/kg
Yield strength (elastic limit)74–92.3MPa
Tensile strength74.9–91.5MPa
Specific strength50.5–63kN.m/kg
Elongation4.98–7.16% strain
Elongation at yield4.19–7.95% strain
Compressive modulus5.46–6.03GPa
Compressive strength94.8–105MPa
Flexural modulus4.83–5.78GPa
Flexural strength (modulus of rupture)111–135MPa
Shear modulus2.05–2.15GPa
Shear strength44.9–54.9MPa
Bulk modulus6.89–7.62GPa
Poisson’s ratio0.347–0.368 
Shape factor6.42
Hardness – Vickers24–26HV
Hardness – Rockwell M132–146 
Hardness – Rockwell R132–146 
Hardness – Shore D86–89 
Elastic stored energy (springs)474–755kJ/m3
Fatigue strength at 10^7 cycles31.6–34.9MPa

PA66 40% Glass and Mineral Impact & fracture properties

Fracture toughness4.35–4.81MPa.m0.5
Toughness (G)3.17–4.24kJ/m2
Impact strength, notched 23 °C4.61–8.94kJ/m2
Impact strength, notched -30 °C2.29–4.98kJ/m2
Impact strength, unnotched 23 °C40.1–58.9kJ/m2
Impact strength, unnotched -30 °C30–45kJ/m2

PA66 40% Glass and Mineral Thermal properties

Melting point250–260°C
Glass temperature54–66°C
Heat deflection temperature 0.45MPa249–258°C
Heat deflection temperature 1.8MPa222–252°C
Maximum service temperature90–130°C
Minimum service temperature-81–-71°C
Thermal conductivity0.443–0.479W/m.°C
Specific heat capacity1320–1380J/kg.°C
Thermal expansion coefficient36–97.2µstrain/°C
Thermal shock resistance147–407°C
Thermal distortion resistance0.00474–0.0128MW/m

PA66 40% Glass and Mineral Electrical properties

Electrical resistivity2.87e19–7.18e20µohm.cm
Electrical conductivity2.4e-19–6.01e-18%IACS
Dielectric constant (relative permittivity)9.96–14 
Dissipation factor (dielectric loss tangent)0.127–0.334 
Dielectric strength (dielectric breakdown)25.9–44.1MV/m
Comparative tracking index375–450V

PA66 40% Glass and Mineral Magnetic properties

Magnetic typeNon-magnetic

PA66 40% Glass and Mineral Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity1860–2090m/s
Mechanical loss coefficient (tan delta)0.0109–0.0121 

PA66 40% Glass and Mineral Absorption & permeability

Water absorption @ 24 hrs0.46–0.74%
Water absorption @ sat4.3–5.7%
Humidity absorption @ sat1.2–1.7%

PA66 40% Glass and Mineral Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.1 – 0.5 %
Melt temperature223 – 310 °C
Molding pressure range61.9 – 138 MPa

PA66 40% Glass and Mineral Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Poor
FlammabilitySlow-burning