PA66 25-30% Mineral Filled Impact Modified Material Data Sheet

PA66 25-30% Mineral Filled Impact Modified (Polyamide 66) Material Data Sheet

PA66 25-30% Mineral Filled Impact Modified Overview

PA66 25-30% mineral filled impact modified is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 25-30% Mineral Filled, Impact Modified). This PA66 25-30% mineral filled impact modified material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.

PA66 25-30% Mineral Filled Impact Modified Designation

Polyamide (Nylon) (Type 66, 25-30% Mineral Filled, Impact Modified)
TradenamesMinlon, Radilon, Schulamid, Wellamid

PA66 25-30% Mineral Filled Impact Modified Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA66 25-30% Mineral Filled Impact Modified Composition detail

Polymer55–72%
Impact modifier3–15%
Mineral (unspecified)25–30%

PA66 25-30% Mineral Filled Impact Modified Physical properties

Density1.35–1.37g/cm3

PA66 25-30% Mineral Filled Impact Modified Mechanical properties

Young’s modulus1.54–1.91GPa
Specific stiffness1.13–1.4MN.m/kg
Yield strength (elastic limit)31.2–38.9MPa
Tensile strength52.2–63.8MPa
Specific strength22.9–28.6kN.m/kg
Elongation32.8–47.2% strain
Elongation at yield13.1–24.9% strain
Compressive modulus1.64–1.81GPa
Compressive strength66.1–73.1MPa
Flexural modulus1.18–1.42GPa
Flexural strength (modulus of rupture)73.8–90.2MPa
Shear modulus0.605–0.636GPa
Shear strength31.3–38.3MPa
Bulk modulus2.48–2.74GPa
Poisson’s ratio0.375–0.39 
Shape factor5.3
Hardness – Vickers10–11HV
Hardness – Rockwell M109–120 
Hardness – Rockwell R109–120 
Hardness – Shore D80–83 
Elastic stored energy (springs)281–446kJ/m3
Fatigue strength at 10^7 cycles22–24.4MPa

PA66 25-30% Mineral Filled Impact Modified Impact & fracture properties

Fracture toughness3.42–3.77MPa.m0.5
Toughness (G)6.53–8.66kJ/m2
Impact strength, notched 23 °C6.77–13.1kJ/m2
Impact strength, notched -30 °C2.61–5.69kJ/m2
Impact strength, unnotched 23 °C166–244kJ/m2
Impact strength, unnotched -30 °C58–87kJ/m2

PA66 25-30% Mineral Filled Impact Modified Thermal properties

Melting point250–260°C
Glass temperature54–66°C
Heat deflection temperature 0.45MPa204–238°C
Heat deflection temperature 1.8MPa149–238°C
Maximum service temperature57–77°C
Minimum service temperature-81–-71°C
Thermal conductivity0.333–0.347W/m.°C
Specific heat capacity1420–1480J/kg.°C
Thermal expansion coefficient52.9–55.1µstrain/°C
Thermal shock resistance323–438°C
Thermal distortion resistance0.00613–0.00648MW/m

PA66 25-30% Mineral Filled Impact Modified Electrical properties

Electrical resistivity2e20–5e21µohm.cm
Electrical conductivity3.45e-20–8.62e-19%IACS
Dielectric constant (relative permittivity)7.76–10.9 
Dissipation factor (dielectric loss tangent)0.127–0.334 
Dielectric strength (dielectric breakdown)31.8–54.2MV/m
Comparative tracking index550  V

PA66 25-30% Mineral Filled Impact Modified Magnetic properties

Magnetic typeNon-magnetic

PA66 25-30% Mineral Filled Impact Modified Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity1060–1190m/s
Mechanical loss coefficient (tan delta)0.022–0.0244 

PA66 25-30% Mineral Filled Impact Modified Absorption & permeability

Water absorption @ 24 hrs0.51–0.83%
Water absorption @ sat5–6.6%
Humidity absorption @ sat1.5–2.1%

PA66 25-30% Mineral Filled Impact Modified Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage1 – 1.8 %
Melt temperature218 – 299 °C
Mold temperature70 – 100 °C
Molding pressure range68.8 – 138 MPa

PA66 25-30% Mineral Filled Impact Modified Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Poor
FlammabilitySlow-burning