PA66 Lubricated 10% PTFE Material Data Sheet

PA66 Lubricated 10% PTFE (Polyamide 66) Material Data Sheet

PA66 Lubricated 10% PTFE Overview

PA66 lubricated 10% PTFE is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, Lubricated, 10% PTFE). This PA66 lubricated 10% PTFE material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.

PA66 Lubricated 10% PTFE Designation

Polyamide (Nylon) (Type 66, Lubricated, 10% PTFE)
TradenamesAlcom, Ashlene, Bestnyl, Chemlon, Clariant, Delta, Eplamid, Hifill, Hylon, Hyundai, Latilub, LNP Lubricomp, LNP Lubriloy, Lubemid, Lubricomp, Lubrione, Luvocom, Nilamid, Nymax, Nypol, Oxnilon, Plaslube, Plustek, Polynil, Pryme, Radici, Spartech, Terez, Torzen, Tribocomp, Trimid, Vydyne, Zytel

PA66 Lubricated 10% PTFE Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA66 Lubricated 10% PTFE Composition detail

Polymer90  %
PTFE (lubricant)10  %

PA66 Lubricated 10% PTFE Physical properties

Density1.18–1.2g/cm3

PA66 Lubricated 10% PTFE Mechanical properties

Young’s modulus1.17–1.46GPa
Specific stiffness0.983–1.23MN.m/kg
Yield strength (elastic limit)35.6–44.4MPa
Tensile strength43.2–52.8MPa
Specific strength29.9–37.3kN.m/kg
Elongation25.3–36.3% strain
Elongation at yield11.7–22.2% strain
Compressive modulus1.25–1.38GPa
Compressive strength54.7–60.4MPa
Flexural modulus1.26–1.51GPa
Flexural strength (modulus of rupture)45–55.1MPa
Shear modulus0.458–0.481GPa
Shear strength25.9–31.7MPa
Bulk modulus2.13–2.35GPa
Poisson’s ratio0.386–0.402 
Shape factor4.3
Hardness – Vickers11–13HV
Hardness – Rockwell M98–108 
Hardness – Rockwell R98–108 
Hardness – Shore D76–79 
Elastic stored energy (springs)479–763kJ/m3
Fatigue strength at 10^7 cycles18.2–20.1MPa

PA66 Lubricated 10% PTFE Impact & fracture properties

Fracture toughness3.23–3.57MPa.m0.5
Toughness (G)7.63–10.2kJ/m2
Impact strength, notched 23 °C6.4–7kJ/m2
Impact strength, notched -30 °C3.3–7.18kJ/m2
Impact strength, unnotched 23 °C55–74.7kJ/m2

PA66 Lubricated 10% PTFE Thermal properties

Melting point260–265°C
Glass temperature54–66°C
Heat deflection temperature 0.45MPa96–133°C
Heat deflection temperature 1.8MPa71–106°C
Maximum service temperature90–130°C
Minimum service temperature-81–-71°C
Thermal conductivity0.281–0.292W/m.°C
Specific heat capacity1530–1600J/kg.°C
Thermal expansion coefficient79.4–82.6µstrain/°C
Thermal shock resistance322–438°C
Thermal distortion resistance0.00344–0.00363MW/m

PA66 Lubricated 10% PTFE Electrical properties

Electrical resistivity5.37e19–1.34e21µohm.cm
Electrical conductivity1.29e-19–3.21e-18%IACS
Dielectric constant (relative permittivity)5.55–7.82 
Dissipation factor (dielectric loss tangent)0.0684–0.18 
Dielectric strength (dielectric breakdown)32.3–55MV/m
Comparative tracking index600  V

PA66 Lubricated 10% PTFE Magnetic properties

Magnetic typeNon-magnetic

PA66 Lubricated 10% PTFE Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity990–1110m/s
Mechanical loss coefficient (tan delta)0.0213–0.0236 

PA66 Lubricated 10% PTFE Absorption & permeability

Water absorption @ 24 hrs0.55–0.9%
Water absorption @ sat6.3–8.4%
Humidity absorption @ sat1.8–2.5%

PA66 Lubricated 10% PTFE Processing properties

Polymer injection moldingLimited use
Polymer extrusionUnsuitable
Polymer thermoformingLimited use
Linear mold shrinkage0.91 – 1.1 %
Melt temperature223 – 299 °C
Mold temperature70 – 100 °C
Molding pressure range6.88 – 103 MPa

PA66 Lubricated 10% PTFE Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Poor
FlammabilitySlow-burning