PA66 Toughened Grade Material Data Sheet

PA66 Toughened Grade (Polyamide 66) Material Data Sheet

PA66 Toughened Grade Overview

PA66 toughened grade is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, Unreinforced, Toughened). This PA66 toughened grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.

PA66 Toughened Grade Designation

Polyamide (Nylon) (Type 66, Unreinforced, Toughened)
TradenamesAltech, Amilan, Anjatech, Aquamid, Badamid, Bestnyl, Chemlon, Durethan, Ecotan, Kepamid, Kopa, Leona, Maxamid, Nylene, Nylfor, Nyloy, Nymax, Omnilon, Pentamid, Plustek, Radici, Radilon, Schulamid, Slovamid, Staramide, Taromid, Technyl, Tecomid, Thermotuf, Thermylon, Torzen, Ultramid, Vitamide, Vydyne, Wellamid, Zytel

PA66 Toughened Grade Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA66 Toughened Grade Composition detail

Polymer85–97%
Impact modifier3–15%

PA66 Toughened Grade Physical properties

Density1.06–1.08g/cm3

PA66 Toughened Grade Mechanical properties

Young’s modulus0.939–1.17GPa
Specific stiffness0.877–1.09MN.m/kg
Yield strength (elastic limit)36.1–45.1MPa
Tensile strength41.6–50.8MPa
Specific strength33.7–42.2kN.m/kg
Elongation41–59% strain
Elongation at yield18.1–34.4% strain
Compressive modulus1–1.11GPa
Compressive strength52.7–58.2MPa
Flexural modulus0.755–0.905GPa
Flexural strength (modulus of rupture)30.2–36.9MPa
Shear modulus0.378–0.397GPa
Shear strength24.9–30.5MPa
Bulk modulus1.19–1.32GPa
Poisson’s ratio0.34–0.36 
Shape factor3.88
Hardness – Vickers12–13HV
Hardness – Rockwell M48–53 
Hardness – Rockwell R91–100 
Hardness – Brinell76–94HB
Hardness – Shore D76–79 
Elastic stored energy (springs)615–981kJ/m3
Fatigue strength at 10^7 cycles17.6–19.4MPa

PA66 Toughened Grade Impact & fracture properties

Fracture toughness3.09–3.42MPa.m0.5
Toughness (G)8.72–11.7kJ/m2
Impact strength, notched 23 °C84.2–163kJ/m2
Impact strength, notched -30 °C14.1–30.6kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2
Impact strength, unnotched -30 °C590–600kJ/m2

PA66 Toughened Grade Thermal properties

Melting point240–265°C
Glass temperature54–66°C
Heat deflection temperature 0.45MPa196–228°C
Heat deflection temperature 1.8MPa60–79°C
Maximum service temperature37–52°C
Minimum service temperature-81–-71°C
Thermal conductivity0.24–0.32W/m.°C
Specific heat capacity1650–1710J/kg.°C
Thermal expansion coefficient141–147µstrain/°C
Thermal shock resistance229–312°C
Thermal distortion resistance0.00167–0.00223MW/m

PA66 Toughened Grade Electrical properties

Electrical resistivity5.37e19–1.34e21µohm.cm
Electrical conductivity1.29e-19–3.21e-18%IACS
Dielectric constant (relative permittivity)5.55–7.82 
Dissipation factor (dielectric loss tangent)0.0684–0.18 
Dielectric strength (dielectric breakdown)32.3–55MV/m
Comparative tracking index575–600V

PA66 Toughened Grade Magnetic properties

Magnetic typeNon-magnetic

PA66 Toughened Grade Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity935–1050m/s
Mechanical loss coefficient (tan delta)0.0276–0.0305 

PA66 Toughened Grade Absorption & permeability

Water absorption @ 24 hrs0.55–0.89%
Water absorption @ sat5.7–7.6%
Humidity absorption @ sat1.8–2.4%
Water vapor transmission0.865–1.46g.mm/m².day
Permeability (O2)0.339–0.995cm³.mm/m².day.atm

PA66 Toughened Grade Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage1.2 – 1.8 %
Melt temperature223 – 304 °C
Mold temperature60 – 80 °C
Molding pressure range6.88 – 138 MPa

PA66 Toughened Grade Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisAcceptable
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Poor
FlammabilitySlow-burning